Home » PA (Polyamide / Nylon) » PA6 (Polyamide 6 / Nylon 6) » PA6 Unfilled Grades » PA6 Lubricated 5% MoS2 Material Data Sheet
PA6 Lubricated 5% MoS2 (Polyamide 6) Material Data Sheet
PA6 Lubricated 5% MoS2 Overview
PA6 lubricated 5% MoS2 is a grade of polyamide 6 (PA6, nylon 6), designated Polyamide (Nylon) (Type 6, MoS2 Lubricated, Anti-friction). This PA6 lubricated 5% MoS2 material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA6 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA6 parts in-house and inspects them before shipment.
PA6 Lubricated 5% MoS2 Designation
Polyamide (Nylon) (Type 6, MoS2 Lubricated, Anti-friction) Tradenames Aegis, Akulon, Alphalon, Ashlene, Bestnyl, Chemlon, Denilub, Eplamid, Firestone, Hifill, Hylon, Hyundai, Kepamid, Latilub, Lubemid, Lubriblend, Nycal, Nycast, Nylene, Pentamid, Plaslube, Promyde, Pryme, Quadrant, Radici, Star, Tecast, Terez, Ultramid, Vitamide
PA6 Lubricated 5% MoS2 Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA6 Lubricated 5% MoS2 Composition detail
Polymer 95 – 96 % MoS2 (molybdenum disulfide) 4 – 5 %
PA6 Lubricated 5% MoS2 Physical properties
PA6 Lubricated 5% MoS2 Mechanical properties
Young’s modulus 0.979 – 1.22 GPa Specific stiffness 0.866 – 1.08 MN.m/kg Yield strength (elastic limit) 44.5 – 55.5 MPa Tensile strength 53.9 – 65.9 MPa Specific strength 39.4 – 49.1 kN.m/kg Elongation 37.2 – 53.5 % strain Elongation at yield 15.2 – 28.8 % strain Compressive modulus 1.05 – 1.16 GPa Compressive strength 68.3 – 75.5 MPa Flexural modulus 0.4 – 0.479 GPa Flexural strength (modulus of rupture) 39.8 – 48.6 MPa Shear modulus 0.394 – 0.415 GPa Shear strength 32.3 – 39.5 MPa Bulk modulus 1.24 – 1.38 GPa Poisson’s ratio 0.34 – 0.36 Shape factor 3.6 Hardness – Vickers 14 – 16 HV Hardness – Rockwell M 111 – 122 Hardness – Rockwell R 111 – 122 Hardness – Shore D 80 – 83 Elastic stored energy (springs) 896 – 1420 kJ/m3 Fatigue strength at 10^7 cycles 22.8 – 25.2 MPa
PA6 Lubricated 5% MoS2 Impact & fracture properties
Fracture toughness 3.12 – 3.45 MPa.m0.5 Toughness (G) 8.52 – 11.4 kJ/m2 Impact strength, notched 23 °C 40.8 – 79.2 kJ/m2 Impact strength, notched -30 °C 3.09 – 6.72 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
PA6 Lubricated 5% MoS2 Thermal properties
Melting point 210 – 220 °C Glass temperature 44 – 56 °C Heat deflection temperature 0.45MPa 92 – 129 °C Heat deflection temperature 1.8MPa 76 – 112 °C Maximum service temperature 90 – 130 °C Minimum service temperature -64 – -54 °C Thermal conductivity 0.283 – 0.295 W/m.°C Specific heat capacity 1560 – 1620 J/kg.°C Thermal expansion coefficient 89.1 – 90.9 µstrain/°C Thermal shock resistance 434 – 589 °C Thermal distortion resistance 0.00314 – 0.00328 MW/m
PA6 Lubricated 5% MoS2 Electrical properties
Electrical resistivity 2e17 – 5e18 µohm.cm Electrical conductivity 3.45e-17 – 8.62e-16 %IACS Dielectric constant (relative permittivity) 7.3 – 10.3 Dissipation factor (dielectric loss tangent) 0.091 – 0.24 Dielectric strength (dielectric breakdown) 28.9 – 49.1 MV/m Comparative tracking index 600 V
PA6 Lubricated 5% MoS2 Magnetic properties
Magnetic type Non-magnetic
PA6 Lubricated 5% MoS2 Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 929 – 1040 m/s Mechanical loss coefficient (tan delta) 0.0379 – 0.0419
PA6 Lubricated 5% MoS2 Absorption & permeability
Water absorption @ 24 hrs 1.9 – 3 % Water absorption @ sat 8.2 – 11 % Humidity absorption @ sat 1.8 – 2.4 %
PA6 Lubricated 5% MoS2 Processing properties
Polymer injection molding Excellent Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 1 – 1.2 % Melt temperature 186 – 260 °C Mold temperature 40 – 60 °C Molding pressure range 34.4 – 138 MPa
PA6 Lubricated 5% MoS2 Durability
Water (fresh) Excellent Water (salt) Acceptable Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Limited use Strong alkalis Limited use Organic solvents Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning