PEKK 30% Glass Fiber (Polyetherketoneketone) Material Data Sheet
PEKK 30% Glass Fiber Overview
PEKK 30% glass fiber is a grade of polyetherketoneketone (PEKK), designated Polyetherketoneketone (30% glass fiber). This PEKK 30% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEKK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEKK parts in-house and inspects them before shipment.
PEKK Designation
Polyetherketoneketone (30% glass fiber) Tradenames Oxpekk
PEKK 30% Glass Fiber Composition detail
Polymer 70 % Glass (fiber) 30 %
PEKK Physical properties
PEKK 30% Glass Fiber Mechanical properties
Young’s modulus 11.8 – 12.6 GPa Specific stiffness 7.78 – 8.34 MN.m/kg Yield strength (elastic limit) 144 – 153 MPa Tensile strength 177 – 188 MPa Specific strength 95.2 – 101 kN.m/kg Elongation 1.75 – 1.98 % strain Elongation at yield 1.8 – 2 % strain Compressive modulus 11.8 – 12.6 GPa Compressive strength 209 – 231 MPa Flexural modulus 10.7 – 11.3 GPa Flexural strength (modulus of rupture) 253 – 261 MPa Shear modulus 4.4 – 4.7 GPa Shear strength 80 – 89 MPa Poisson’s ratio 0.41 – 0.45 Shape factor 7.18 Hardness – Vickers 43 – 45 HV Hardness – Rockwell M 98 – 108 Elastic stored energy (springs) 846 – 970 kJ/m3 Fatigue strength at 10^7 cycles 69.4 – 76.7 MPa
PEKK Impact & fracture properties
Impact strength, notched 23 °C 8.62 – 9.74 kJ/m2 Impact strength, unnotched 23 °C 72.1 – 88.1 kJ/m2
PEKK 30% Glass Fiber Thermal properties
Melting point 347 – 373 °C Glass temperature 159 – 163 °C Heat deflection temperature 0.45MPa 324 – 330 °C Heat deflection temperature 1.8MPa 316 – 322 °C Vicat softening point 324 – 330 °C Maximum service temperature 233 – 287 °C Thermal conductivity 0.422 – 0.458 W/m.°C Specific heat capacity 1310 – 1340 J/kg.°C Thermal expansion coefficient 15.6 – 16.4 µstrain/°C Thermal shock resistance 725 – 803 °C Thermal distortion resistance 0.0262 – 0.0288 MW/m
PEKK Electrical properties
Electrical resistivity 9249999999999999475712 – 10800000000000000000000 µohm.cm Electrical conductivity 1.6e-20 – 1.86e-20 %IACS Dielectric constant (relative permittivity) 3.17 – 3.43 Dissipation factor (dielectric loss tangent) 0.0035 – 0.0045 Dielectric strength (dielectric breakdown) 23 – 25 MV/m
PEKK Magnetic properties
Magnetic type Non-magnetic
PEKK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2790 – 2890 m/s
PEKK Absorption & permeability
Water absorption @ 24 hrs 0.063 – 0.077 %
PEKK Processing properties
Polymer injection molding Acceptable Polymer extrusion Limited use Polymer thermoforming Unsuitable Linear mold shrinkage 0.25 – 0.35 % Melt temperature 376 – 383 °C Mold temperature 132 – 249 °C Molding pressure range 103 – 138 MPa
PEKK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Unacceptable Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oils and fuels Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Excellent Flammability Self-extinguishing