Nickel-Fe-Cr alloy, NIMONIC PE16, bar
NIMONIC PE16 Designation
| INCO Inc. | Proprietary Alloy: “NIMONIC PE16” |
NIMONIC PE16 Tradenames
| NIMONIC PE16 | Special Metals Corp. (USA) |
NIMONIC PE16 Typical uses
NIMONIC PE16 Composition detail
| Al (aluminum) | 1 | | | % |
| Cr (chromium) | 16.5 | | | % |
| Fe (iron) | 34.4 | | | % |
| Mo (molybdenum) | 3.2 | | | % |
| Ni (nickel) | 43.5 | | | % |
| Ti (titanium) | 1.2 | | | % |
| Other | 0 | – | 0.1 | % |
NIMONIC PE16 Physical properties
NIMONIC PE16 Mechanical properties
| Young’s modulus | 195 | – | 205 | GPa |
| Specific stiffness | 24.3 | – | 25.6 | MN.m/kg |
| Yield strength (elastic limit) | 460 | – | 585 | MPa |
| Tensile strength | 795 | – | 975 | MPa |
| Specific strength | 57.3 | – | 72.9 | kN.m/kg |
| Elongation | 30 | – | 45 | % strain |
| Compressive strength | 460 | – | 585 | MPa |
| Flexural modulus | 195 | – | 205 | GPa |
| Flexural strength (modulus of rupture) | 460 | – | 585 | MPa |
| Shear modulus | 75 | – | 85 | GPa |
| Bulk modulus | 145 | – | 175 | GPa |
| Poisson’s ratio | 0.28 | – | 0.3 | |
| Shape factor | 25 | | | |
| Hardness – Vickers | 270 | – | 310 | HV |
| Hardness – Rockwell B | 103 | – | 106 | HRB |
| Hardness – Rockwell C | 26 | – | 31 | HRC |
| Hardness – Brinell | 256 | – | 294 | HB |
| Elastic stored energy (springs) | 536 | – | 846 | kJ/m3 |
| Fatigue strength at 10^7 cycles | 315 | – | 490 | MPa |
Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles | 294 | – | 525 | MPa |
NIMONIC PE16 Impact & fracture properties
| Fracture toughness | 215 | – | 239 | MPa.m0.5 |
| Toughness (G) | 231 | – | 285 | kJ/m2 |
NIMONIC PE16 Thermal properties
| Melting point | 1230 | – | 1380 | °C |
| Maximum service temperature | 697 | – | 967 | °C |
| Minimum service temperature | -273 | | | °C |
| Thermal conductivity | 11 | – | 12.5 | W/m.°C |
| Specific heat capacity | 525 | – | 565 | J/kg.°C |
| Thermal expansion coefficient | 10.5 | – | 12.5 | µstrain/°C |
| Thermal shock resistance | 195 | – | 262 | °C |
| Thermal distortion resistance | 0.92 | – | 1.14 | MW/m |
| Latent heat of fusion | 270 | – | 300 | kJ/kg |
NIMONIC PE16 Electrical properties
| Electrical resistivity | 105 | – | 115 | µohm.cm |
| Electrical conductivity | 1.5 | – | 1.64 | %IACS |
| Galvanic potential | -0.13 | – | -0.05 | V |
NIMONIC PE16 Magnetic properties
| Magnetic type | Non-magnetic |
NIMONIC PE16 Optical, aesthetic and acoustic properties
| Transparency | Opaque |
| Acoustic velocity | 4930 | – | 5060 | m/s |
| Mechanical loss coefficient (tan delta) | 3e-4 | – | 5e-4 | |
NIMONIC PE16 Processing properties
| Metal casting | Unsuitable |
| Metal cold forming | Acceptable |
| Metal hot forming | Acceptable |
| Metal press forming | Acceptable |
| Metal deep drawing | Unsuitable |
| Machining speed | 5.79 m/min |
Weldability Notes: Preheating is not required, post weld heat treatment is required | Good |
NIMONIC PE16 Durability
| Water (fresh) | Excellent |
| Water (salt) | Excellent |
| Weak acids | Excellent |
| Strong acids | Acceptable |
| Weak alkalis | Excellent |
| Strong alkalis | Excellent |
| Organic solvents | Excellent |
| Oxidation at 500C | Excellent |
| UV radiation (sunlight) | Excellent |
Galling resistance (adhesive wear) Notes: Bronze or zinc alloy dies should be used to minimize galling. | Limited use |
| Flammability | Non-flammable |
NIMONIC PE16 Corrosion resistance
| Pitting resistance equivalent number (PREN) | 27.1 |
| Pitting and crevice corrosion | Medium (20-30) |
Stress corrosion cracking Note: Rated in chloride; Other susceptible environments: Hydroxide | Slightly susceptible |
NIMONIC PE16 Notes
| Warning |
| All nickel compounds should be regarded as toxic. Some can cause cancer and/or fetal abnormalities. |
| Other notes |
| NIMONIC is a registered tradename of the INCO group of companies. |
NIMONIC PE16 Standards with similar compositions
| Tradenames: NIMONIC PE 16 |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey