NIMONIC 942 (bar) Material Data Sheet
Nickel-Fe-Cr alloy, NIMONIC 942, bar NIMONIC 942 Designation INCO Inc. Proprietary Alloy: “NIMONIC 942” NIMONIC 942 Tradenames NIMONIC 942 Special Metals Corp. (USA) NIMONIC 942 Typical uses Aerospace NIMONIC 942 Compositional summary Ni50 / Fe27 / Cr12 / Mo6 / Ti3.7 / Al1 / Si0.3 / Mn0.2 (impurities: Other<0.1) Material family Metal (non-ferrous) Base material … Continue reading NIMONIC 942 (bar) Material Data Sheet