AISI 205 Stainless Steel Thermal Properties
| Melting point | 1400 | – | 1450 | °C |
| Maximum service temperature | 755 | – | 787 | °C |
| Minimum service temperature | -150 | °C | ||
| Thermal conductivity | 15 | – | 17 | W/m.°C |
| Specific heat capacity | 490 | – | 530 | J/kg.°C |
| Thermal expansion coefficient | 17.1 | – | 19.1 | µstrain/°C |
| Thermal shock resistance | 118 | – | 150 | °C |
| Thermal distortion resistance | 0.814 | – | 0.96 | MW/m |
| Latent heat of fusion | 260 | – | 285 | kJ/kg |
AISI 205 Stainless Steel Designation
| AISI 205, wrought |
| UNS number S20500 |
| US name ASTM S20500 |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey