AISI 205 Stainless Steel, Annealed, Mechanical Properties
AISI 205 Stainless Steel, Annealed, Mechanical Properties Young’s modulus 193 – 201 GPa Specific stiffness 24.7 – 25.9 MN.m/kg Yield strength (elastic limit) 425 – 525 MPa Tensile strength 745 – 925 MPa Specific strength 54.5 – 67.4 kN.m/kg Elongation 40 – 70 % strain Compressive strength 425 – 525 MPa Flexural modulus 193 – … Continue reading AISI 205 Stainless Steel, Annealed, Mechanical Properties