ADI 1600 Austempered Ductile Cast Iron Mechanical Properties

ADI 1600 Mechanical properties

Young’s modulus155–163GPa
Specific stiffness21.9–23.1MN.m/kg
Yield strength (elastic limit)1260–1470MPa
Tensile strength1600–1770MPa
Specific strength178–208kN.m/kg
Elongation1–2% strain
Compressive modulus155–163GPa
Compressive strength2340–2710MPa
Flexural modulus155–163GPa
Flexural strength (modulus of rupture)1410–1560MPa
Shear modulus57.2–67.1GPa
Shear strength1370–1600MPa
Bulk modulus101–107GPa
Poisson’s ratio0.24–0.25 
Shape factor2   
Hardness – Vickers444–490HV
Hardness – Brinell444–490HB
Elastic stored energy (springs)5010–6770kJ/m^3
Fatigue strength at 10^7 cycles444–518MPa

ADI 1600 Impact & fracture properties

Fracture toughness 40–48MPa.m^0.5
Toughness (G) 10.1–14.4kJ/m^2

ADI 1600 Designation

ADI 1600
Condition                                                                                              Cast and austempered

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey