ADI 1600 Austempered Ductile Cast Iron Thermal Properties

ADI 1600 Thermal Properties Melting point 1110 – 1190 °C Maximum service temperature 350 – 450 °C Minimum service temperature 0     °C Thermal conductivity 20.1 – 21.7 W/m.°C Specific heat capacity 460 – 495 J/kg.°C Thermal expansion coefficient 11.5 – 15.5 µstrain/°C Thermal shock resistance 543 – 758 °C Thermal distortion resistance 1.34 … Continue reading ADI 1600 Austempered Ductile Cast Iron Thermal Properties