Bronze CuAl10Ni5Fe4Mn1 Similar Compositions (C95800, cast aluminum bronze)

Designation
C95800 (Nickel Aluminum Bronze)
ConditionAs cast
UNS numberC95800
US nameC95800 to ASTM B30, ASTM B505, ASTM B763, ASTM B806, ASTM B148, SAE J462
EN name2.0976, GB-CuAl10Ni to DIN 17656;  U-A9N5FeY200 to NF A53-709
JIS (Japanese) nameAlBC3, AlBC3C, CAC703 to JIS H5114, JIS H5121;  AlBCIn2 to JIS H2206

Bronze CuAl10Ni5Fe4Mn1 Equivalent Grades (C95800, cast aluminum bronze)

C95800 to ASTM B30, ASTM B505, ASTM B763, ASTM B806, ASTM B148, SAE J462
2.0976, GB-CuAl10Ni to DIN 17656
U-A9N5FeY200 to NF A53-709
AlBC3, AlBC3C, CAC703 to JIS H5114, JIS H5121
AlBCIn2 to JIS H2206
5716-15 to SIS 145716
CuAl10Ni6Fe4 to SABS 200
16570 to NS 16570
Ampco 483, MTEK 230-N

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey