Bronze CuAl10Ni5Fe4Mn1 Chemical Composition (C95800, cast aluminum bronze)

Designation
C95800 (Nickel Aluminum Bronze)
ConditionAs cast
UNS numberC95800
US nameC95800 to ASTM B30, ASTM B505, ASTM B763, ASTM B806, ASTM B148, SAE J462
EN name2.0976, GB-CuAl10Ni to DIN 17656;  U-A9N5FeY200 to NF A53-709
JIS (Japanese) nameAlBC3, AlBC3C, CAC703 to JIS H5114, JIS H5121;  AlBCIn2 to JIS H2206

Bronze CuAl10Ni5Fe4Mn1 Chemical Composition (C95800, cast aluminum bronze)

Al (aluminum)8.5–9.5%
Cr (chromium)0–0.01%
Cu (copper)79–83.2%
Fe (iron)3.5–4.5%
Mn (manganese)0.8–1.5%
Ni (nickel)4–5%
Pb (lead)0–0.03%
Si (silicon)0–0.1%
Sn (tin)0–0.1%
Zn (zinc)0–0.2%

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey