Modulus Metal | Manufacturer Company in TURKEY: Sand Casting | Investment Casting | Foundry | CNC Machining | Press Bending | Laser Cutting | Welding | Plastics Injection Molding |Turkiye Fracture Toughness & Toughness Values Fracture toughness 60 – 75 MPa.m^0.5 Toughness (G) * 18.1 – 28 kJ/m^2 *Values indicated with asterisks (*) are approximate. No … Continue reading AISI 202 Stainless steel (Low nickel general purpose), austenitic, Annealed | Toughness | Fracture Toughness