Low Carbon steel, AISI 1025 annealed (Plain Carbon, 0.25%C) Equivalent Grades | Sand Casting | Investment Casting | Foundry | CNC Machining | Supplier Company | Modulus Metal in TURKEY

Low Carbon Steel General Info

The most affordable of all structural metals is low-carbon steel, usually referred to as mild steel. It is utilized extensively for a variety of purposes.

Strengths
Very low cost, superior to higher carbon steels in terms of toughness, machinability, formability, and weldability. Cold-working improves machinability and strength.

Limitations
Low strength and poor hardenability as compared to higher carbon steels.

Designation
The AISI/SAE designations for carbon steels are 10xx, 11xx, 12xx, and 15xx. Low carbon steels have carbon contents as indicated by the last two numbers, which can reach 30. The EN designations 1.03zz and 1.04zz apply to low carbon steels.

Common uses
Numerous applications, including the reinforcement of concrete, building sections, roofing sheets, vehicle body panels, and cans.

Low Carbon steel, AISI 1025 annealedEquivalent Grades
UNS numberG10250
US nameASME 1025, ASTM M1025, ASTM 1025, ASME G10250, SAE 850, AMS 5045, ~SAE 853 Class 1 Type 5, ~SAE 853 Class 1 Type 4, ~SAE 853 Class 1 Type 3, ~SAE 853 Class 1 Type 2, ~SAE 853 Class 1 Type 1, ~SAE 040S, ~SAE 040C, ~SAE 040B, ~SAE 040A, ~ASTM FPA
EN nameS270GP
EN number1.0023
GB (Chinese) name~ML25Mn
JIS (Japanese) nameSWH 400L, SWH 400, STW 400, STW 370, STPY 400, STKR 400, STKN400W, STK400, SSC 400, SKY 400, SKK 400, SDP2G, SDP2, SDP1TG, SDP1T, ~STPL 380, ~STPG 370, ~STKM13C, ~STKM13B, ~STKM13A, ~STC 590 A, ~STC 510 A, ~STC 440, ~STC 370, ~SPHT 3, ~SM400A
Carbon steel, AISI 1025, annealed Equivalent Grades,Sand Casting,Investment Casting,Machining, Turkey,Modulus Metal

Low Carbon steel, AISI 1022 annealed (Plain Carbon, 0.22%C) Equivalent Grades | Sand Casting | Investment Casting | Foundry | CNC Machining | Supplier Company | Modulus Metal in TURKEY

Carbon steel, AISI 1022, annealed Equivalent Grades,Sand Casting,Investment Casting,Machining, Turkey,Modulus Metal

Low Carbon Steel General Info

The most affordable of all structural metals is low-carbon steel, usually referred to as mild steel. It is utilized extensively for a variety of purposes.

Strengths
Very low cost, superior to higher carbon steels in terms of toughness, machinability, formability, and weldability. Cold-working improves machinability and strength.

Limitations
Low strength and poor hardenability as compared to higher carbon steels.

Designation
The AISI/SAE designations for carbon steels are 10xx, 11xx, 12xx, and 15xx. Low carbon steels have carbon contents as indicated by the last two numbers, which can reach 30. The EN designations 1.03zz and 1.04zz apply to low carbon steels.

Common uses
Numerous applications, including the reinforcement of concrete, building sections, roofing sheets, vehicle body panels, and cans.

Low Carbon steel, AISI 1022 annealedEquivalent Grades
UNS numberG10220
US nameASTM MTX1020, ASTM 1022, ASME G10220, ASME G10210, ~SAE 050W, ~SAE 045Z, ~SAE 045Y, ~SAE 045X, ~SAE 045W, ~SAE 040S, ~SAE 040C, ~SAE 040B, ~SAE 040A
EN name2C22, 055M15, ~S270GP
EN number~1.0023
ISO name~R44, ~HR275 Class B, ~E275 Quality A
GB (Chinese) name~ML22Mn
JIS (Japanese) name~SWRCH22A, ~STK500, ~SNR400A, ~SN 400 A ~SM400A, ~SHK 400 M, ~SG 295