ACIER AU CARBONE ET ACIER AU CARBONE MANGANÈSE. EN 10027-1 vs EN 10027-2 vs DIN 17100 Désignation de la nuance d’acier

Modulus Metal | Découpe laser de métal – Pliage – Soudage – Fournisseur de pièces de fabrication en Turquie

Selon
EN 10027-1
and ECISS IC 10
Selon
EN 10027-2
DIN 17100
S1851.0035St  33
S235JR1.0037St  37-2
S235JRG11.0036USt 37-2
S235JRG21.0038RSt 37-2
S235JO1.0114St 37-3 U
S235J2G31.0116St 37-3 N
S235J2G41.0117—
S275JR1.0044St 44-2
S275JO1.0143St 44-3 U
S275J2G31.0144St 44-3 N
S275J2G41.0145—
S355JR1.0045—
S355JO1.0553St 52-3 U
S355J2G31.0570St  52-3 N
S355J2G41.0577—
S356K2G31.0595—
S355K2G41.0596—
E2951.0050St 50-2
E3351.0060St  60-2
E3601.0070St  70-2
Sand Casting Modulus Metal Investment Casting Foundry Gray Ductile Nodular Products Parts Manufacturing Machining CNC Supplier in Turkey Turkei

PLAIN CARBON AND CARBON-MANGANESE STEEL EN 10027-1 vs EN 10027-2 vs DIN 17100 Steel Grade Designation

Modulus Metal | Metal Laser Cutting – Bending – Welding – Manufacturing Parts Supplier in Turkey

Plain Carbon and Carbon-Manganese Steel Grade Designation as per EN 10027-1, EN 10027-2 and DIN 17100

According to
EN 10027-1
and ECISS IC 10
According to
EN 10027-2
DIN 17100
S1851.0035St  33
S235JR1.0037St  37-2
S235JRG11.0036USt 37-2
S235JRG21.0038RSt 37-2
S235JO1.0114St 37-3 U
S235J2G31.0116St 37-3 N
S235J2G41.0117—
S275JR1.0044St 44-2
S275JO1.0143St 44-3 U
S275J2G31.0144St 44-3 N
S275J2G41.0145—
S355JR1.0045—
S355JO1.0553St 52-3 U
S355J2G31.0570St  52-3 N
S355J2G41.0577—
S356K2G31.0595—
S355K2G41.0596—
E2951.0050St 50-2
E3351.0060St  60-2
E3601.0070St  70-2
Modulus Metal Sand Casting Investment Casting Foundry Pouring Gray Ductile Nodular Products Parts Manufacturing Machining CNC Supplier in Turkey Turquie