Young’s modulus 172 – 180 GPa |
Flexural modulus * 172 – 180 GPa |
Shear modulus 67 – 71 GPa |
Bulk modulus 124 – 137 GPa |
Poisson’s ratio 0.27 – 0.28 |
Shape factor 20 |
Yield strength (elastic limit) 526 – 554 MPa |
Tensile strength 900 – 950 MPa |
Compressive strength * 535 – 563 MPa |
Flexural strength (modulus of rupture) 526 – 554 MPa |
Elongation 2 – 5 % strain |
Hardness – Vickers 285 – 300 HV |
Fatigue strength at 10^7 cycles 317 – 324 MPa |
Fatigue strength model (stress range) 227 – 249 MPa Parameters: Stress Ratio = 0, Number of Cycles = 1e7 |
Fracture toughness 22 – 34 MPa.m^0.5 |
Mechanical loss coefficient (tan delta) * 6e-4 – 8e-4 |