EN GJS 800-2 as cast & normalized, nodular graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJS 800-2 as cast & normalized, nodular graphite, Mechanical Properties
Young’s modulus 172 – 180 GPa
Flexural modulus * 172 – 180 GPa
Shear modulus 67 – 71 GPa
Bulk modulus 124 – 137 GPa
Poisson’s ratio 0.27 – 0.28
Shape factor 21
Yield strength (elastic limit) 471 – 526 MPa
Tensile strength 800 – 900 MPa
Compressive strength * 480 – 535 MPa
Flexural strength (modulus of rupture) 471 – 526 MPa
Elongation 2 – 5 % strain
Hardness – Vickers 265 – 290 HV
Fatigue strength at 10^7 cycles 304 – 317 MPa
Fatigue strength model (stress range) 207 – 250 MPa
Parameters: Stress Ratio = 0, Number of Cycles = 1e7
Fracture toughness 22 – 34 MPa.m^0.5
Mechanical loss coefficient (tan delta) * 6e-4 – 0.001
*Values are approximations. This information’s accuracy is not guaranteed.