EN GJS 900-2 hardened & tempered, nodular graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJS 900-2 hardened & tempered, nodular graphite, Mechanical Properties
Young’s modulus 168 – 176 GPa
Flexural modulus * 168 – 176 GPa
Shear modulus 65 – 70 GPa
Bulk modulus 121 – 134 GPa
Poisson’s ratio 0.27 – 0.28
Shape factor 16
Yield strength (elastic limit) 710 – 790 MPa
Tensile strength 900 – 1e3 MPa
Compressive strength * 719 – 799 MPa
Flexural strength (modulus of rupture) 710 – 790 MPa
Elongation 2 – 7 % strain
Hardness – Vickers 290 – 320 HV
Fatigue strength at 10^7 cycles 317 – 330 MPa
Fatigue strength model (stress range) 221 – 263 MPa
Parameters: Stress Ratio = 0, Number of Cycles = 1e7
Fracture toughness 22 – 34 MPa.m^0.5
Mechanical loss coefficient (tan delta) * 6e-4 – 8e-4
*Values are approximations. This information’s accuracy is not guaranteed.
Modulus Metal Sand Casting Investment Casting Foundry Pouring Gray Ductile Iron Nodular Products Parts Manufacturing Machining CNC Supplier in Turkey Turkei Turquie
Sand Casting Molding Moulage Sandguss Au Sable Modulus Metal Turkiye Turkey Turkei Turquie Supplier Fournisseur Lieferant
Sand Casting Modulus Metal Turkey Foundry Supplier Ductile Nodular Gray Grey Iron Steel Casting Company

© Modulus Metal 2017-2022    |    All Rights Reserved