Plain Carbon and Carbon-Manganese Steel Grade Designation as per EN 10027-1, EN 10027-2 and DIN 17100
| According to EN 10027-1 and ECISS IC 10 | According to EN 10027-2 | DIN 17100 |
| S185 | 1.0035 | St 33 |
| S235JR | 1.0037 | St 37-2 |
| S235JRG1 | 1.0036 | USt 37-2 |
| S235JRG2 | 1.0038 | RSt 37-2 |
| S235JO | 1.0114 | St 37-3 U |
| S235J2G3 | 1.0116 | St 37-3 N |
| S235J2G4 | 1.0117 | — |
| S275JR | 1.0044 | St 44-2 |
| S275JO | 1.0143 | St 44-3 U |
| S275J2G3 | 1.0144 | St 44-3 N |
| S275J2G4 | 1.0145 | — |
| S355JR | 1.0045 | — |
| S355JO | 1.0553 | St 52-3 U |
| S355J2G3 | 1.0570 | St 52-3 N |
| S355J2G4 | 1.0577 | — |
| S356K2G3 | 1.0595 | — |
| S355K2G4 | 1.0596 | — |
| E295 | 1.0050 | St 50-2 |
| E335 | 1.0060 | St 60-2 |
| E360 | 1.0070 | St 70-2 |