Modulus Metal | Manufacturer Company in TURKEY: Sand Casting | Investment Casting | Foundry | CNC Machining | Press Bending | Laser Cutting | Welding | Plastics Injection Molding | Engineering | Turkiye | Turkey
| Werkstoff | Germany | U.S.A. | France | Great Britain | Italy | Sweden | Spain | Japan |
|---|---|---|---|---|---|---|---|---|
| No. | DIN | AISI/SAE UNS | AFNOR | BS | UNI | SS | UNE | JIS |
| 1.0332 | St14 | 1008 | 14491CR | 1447 | ||||
| 1.1121 | Ck10 | 1010 | CC10 | 040A10 | 1264 | S10C | ||
| 1.0721 | 10S20 | 1108 | 210M15 | |||||
| 1.0401 | C15 | 1015 | CC12 | 080M15 | C15C16 | 1350 | F.111 | S15C |
| 1.0402 | C22 | 1020 | CC20 | 050A20 | C20C21 | 1450 | F.112 | |
| 1.1141 | Ck15 | 1015 | XC12 | 080M15 | C16 | 1370 | C15K | S15C |
| 1.0036 | USt37-3 | FE37BFU | ||||||
| 1.0715 | 9SMn28 | 1213 | S250 | 230M07 | CF9SMn28 | 1912 | 11SMn28 | SUM22 |
| 1.0718 | 9SMnPb28 | 12L3 | S250Pb | CF9SMnPb28 | 1914 | 11SMnPb28 | SUM22L | |
| 1.0501 | C35 | 1035 | CC35 | 060A35 | C35 | 1550 | F.113 | S35C |
| 1.0503 | C45 | 1045 | CC45 | 080M46 | C45 | 1650 | F.114 | S45C |
| 1.1158 | Ck25 | 1025 | XC25 | 070M25 | C25 | S25C | ||
| 1.1183 | Cf35 | 1035 | XC38TS | 060A35 | C36 | 1572 | S35C | |
| 1.1191 | Ck45 | 1045 | XC42 | 080M46 | C45 | 1672 | C45K | S45C |
| 1.1213 | Cf53 | 1050 | XC48TS | 060A52 | C53 | 1674 | S50C | |
| 1.5415 | 15Mo3 | ASTMA204GrA | 15D3 | 1501-240 | 16Mo3KW | 2912 | 16Mo3 | |
| 1.5423 | 16Mo5 | 4520 | 1503-245-420 | 16Mo5 | 16Mo5 | SB450M | ||
| 1.0050 | St50-2 | FE50 | SM50YA | |||||
| 1.7242 | 16CrMo 4 | 18CrMo4 | 18CrMo4 | |||||
| 1.7337 | 16CrMo 4 4 | A387Gr.12Cl. | A18CrMo45KW | |||||
| 1.7362 | 12CrMo 19 5 | Z10CD5.05 | 3606-625 | 16CrMo205 | ||||
| 1.0060 | St60-2 | FE60-2 | SM570 | |||||
| 1.0535 | C55 | 1055 | 070M55 | C55 | 1655 | S55C | ||
| 1.0601 | C60 | 1060 | CC55 | 080A62 | C60 | S60C | ||
| 1.1203 | Ck55 | 1055 | XC55 | 070M55 | C50 | C55K | S55C | |
| 1.1221 | Ck60 | 1060 | XC60 | 080A62 | C60 | 1678 | S58C | |
| 1.1545 | C1051 | C100KU | SK3 | |||||
| 1.1545 | C105W1 | C100KU | SK3 | |||||
| 1.0070 | St70-2 | FE70-2 | ||||||
| 1.7238 | 49CrMo4 | |||||||
| 1.7561 | 42CrV6 | |||||||
| 1.7701 | 51CrMoV4 | 51CDV4 | 51CrMoV4 |