PARA 30% Carbon Fiber Material Data Sheet

PARA 30% Carbon Fiber (Polyarylamide) Material Data Sheet

PARA 30% Carbon Fiber Overview

PARA 30% carbon fiber is a grade of polyarylamide (PARA), designated Polyarylamide (30% carbon fiber). This PARA 30% carbon fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PARA parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PARA parts in-house and inspects them before shipment.

PARA 30% Carbon Fiber Designation

Polyarylamide (30% carbon fiber)
TradenamesIxef, Reny

PARA 30% Carbon Fiber Composition detail

Polymer70  %
Carbon (fiber)30  %

PARA 30% Carbon Fiber Physical properties

Density1.33–1.36g/cm3

PARA 30% Carbon Fiber Mechanical properties

Young’s modulus22.5–28.1GPa
Specific stiffness16.7–20.9MN.m/kg
Yield strength (elastic limit)188–235MPa
Tensile strength197–241MPa
Specific strength140–175kN.m/kg
Elongation1.04–1.5% strain
Elongation at yield0.879–1.67% strain
Compressive modulus24.1–26.6GPa
Compressive strength250–276MPa
Flexural modulus20.2–24.2GPa
Flexural strength (modulus of rupture)297–363MPa
Shear modulus9.33–9.81GPa
Shear strength118–145MPa
Bulk modulus22.7–25GPa
Poisson’s ratio0.321–0.323 
Shape factor9.27
Hardness – Vickers60–67HV
Hardness – Rockwell M184–204 
Hardness – Rockwell R184–204 
Hardness – Shore D98–102 
Elastic stored energy (springs)695–1110kJ/m3
Fatigue strength at 10^7 cycles83.3–92.1MPa

PARA 30% Carbon Fiber Impact & fracture properties

Fracture toughness5.88–6.49MPa.m0.5
Toughness (G)1.31–1.75kJ/m2
Impact strength, notched 23 °C3.38–6.55kJ/m2
Impact strength, unnotched 23 °C43–47kJ/m2

PARA 30% Carbon Fiber Thermal properties

Melting point269–291°C
Glass temperature78–92.2°C
Heat deflection temperature 0.45MPa247–268°C
Heat deflection temperature 1.8MPa220–240°C
Vicat softening point77–90°C
Maximum service temperature188–207°C
Thermal conductivity0.632–0.648W/m.°C
Specific heat capacity1480–1510J/kg.°C

PARA 30% Carbon Fiber Electrical properties

Electrical resistivity2e20–5e21µohm.cm
Electrical conductivity3.45e-20–8.62e-19%IACS
Dielectric constant (relative permittivity)3.45–5.95 
Dissipation factor (dielectric loss tangent)0.018–0.075 
Dielectric strength (dielectric breakdown)15.7–17.3MV/m
Galvanic potential0.14–0.22V

PARA 30% Carbon Fiber Magnetic properties

Magnetic typeNon-magnetic

PARA 30% Carbon Fiber Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity4080–4580m/s
Mechanical loss coefficient (tan delta)0.00534–0.0059 

PARA 30% Carbon Fiber Absorption & permeability

Water absorption @ 24 hrs0.15–0.25%
Water absorption @ sat3.7–4.9%
Humidity absorption @ sat1.6–2.2%

PARA 30% Carbon Fiber Processing properties

Polymer injection moldingLimited use
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.03 – 0.1 %
Melt temperature269 – 291 °C
Mold temperature116 – 144 °C
Molding pressure range30 – 150 MPa

PARA 30% Carbon Fiber Durability

Water (fresh)Excellent
Water (salt)Acceptable
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisLimited use
Organic solventsLimited use
Oils and fuelsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Good
FlammabilitySlow-burning