| AISI** | DIN | BTS | JIS | UNS | EN | AFNOR | UNI | SIS | Material Number |
| 1013 | USt 34-1 | – | – | G10130 | – | – | – | 1233 | 1.0055 |
| 1010 | C 10 | 045 M 10 | S 10 C | G10100 | C 10 | XC 10 | C 10 | – | 1.0301 |
| 1008 | DD 11 ( StW 22) | HR 3 | SPHD | – | DD 11 | 1 C | – | – | 1.0332 |
| 1020 | C 22 | 050 A 20 | S 22 C | G10200 | 1 C 22 | C 20 | C 20 | 1450 | 1.0402 |
| 1025 | C 25 | 070 M 26 | S 22 C | G10250 | 1 C 25 | C 25 | C 25 | – | 1.0406 |
| 1012 | B 500 H | – | S 12 C | G10120 | B 500 B | XC 12 | B 500 B | 1332 | 1.0439 |
| 1018 | C16.8 | 080 A 17 | – | G10180 | – | – | – | – | 1.0453 |
| 1108 | 10 S 20 | 210 M 15 | – | G 11080 | 10 S 20 | 10 F 1 | CF 10 S 20 | – | 1.0721 |
| 1010 | Ck 10 | 040 A 10 | S 10 C | G10100 | 2 C 10 | XC 10 | C 10 | 1265 | 1.1121 |
| 1022 | 20 Mn 5 | 120 M 19 | SMn 420 | G 10220 | 20 Mn 5 | 20 M 5 | G 22 Mn 3 | – | 1.1133 |
| 1015 | Ck 15 | 080 M 15 | S 15 C | G 10150 | 2 C 15 | XC 15 | C 15 | 1370 | 1.1141 |
| 1021 | 22 B 2 | – | SWRCHB 220 | G10210 | C 22 BE 69 | 21 B 3 | – | – | 1.5508 |
| – | PS 275 TM | S 275 M | – | – | S 275 M | S 275 M | S 275 M | – | 1.8818 |
| – | DI-MC 355 B | – | – | – | S 355 M | E 355 | S 355 M | – | 1.8823 |
| – | DI-MC 420 B | S 420 M | – | – | S 420 M | E 420 | S 420 M | – | 1.8825 |
| – | S 460 M | S 460 M | – | – | S 460 M | E460; S460M | S460M | – | 1.8827 |
| – | BTStE 355 TM | S 355 ML | – | – | S 355 ML | E 355 | S 355 ML | – | 1.8834 |
| – | BTStE 420 TM | S 420 Ml | – | – | S 420 ML | E 420 | S 420 ML | – | 1.8836 |
| – | St E 320-3Z | – | – | – | S 320 GD + ZA | – | – | – | 1.0250 |