INVAR Optical, aesthetic and acoustic properties(cold worked, hard)
Transparency
Opaque
Acoustic velocity
4100
–
4220
m/s
Mechanical loss coefficient (tan delta)
3e-4
–
5e-4
INVAR Processing properties(cold worked, hard)
Metal casting
Unsuitable
Metal cold forming
Excellent
Metal hot forming
Excellent
Metal press forming
Excellent
Metal deep drawing
Unsuitable
Machining speed
11 m/min
Weldability Notes: Preheating is not required, post weld heat treatment is required
Good
INVAR Durability(cold worked, hard)
Water (fresh)
Excellent
Water (salt)
Excellent
Weak acids
Excellent
Strong acids
Acceptable
Weak alkalis
Excellent
Strong alkalis
Excellent
Organic solvents
Excellent
Oxidation at 500C
Excellent
UV radiation (sunlight)
Excellent
Galling resistance (adhesive wear) Notes: Bronze or zinc alloy dies should be used to minimize galling.
Limited use
Flammability
Non-flammable
INVAR Corrosion resistance(cold worked, hard)
Pitting resistance equivalent number (PREN)
0
Pitting and crevice corrosion
Low (<20)
Stress corrosion cracking Note: Rated in chloride; Other susceptible environments: Hydroxide
Not susceptible
INVAR Notes(cold worked, hard)
Warning
INVAR is easy to weld to other metals, but designers must be aware that INVAR’s exceptionally low thermal expansion coefficient may cause problems, if a good match with the thermal properties of the other metal is required.
INVAR Other notes
INVAR is a trademark of Societe Creusot-Loire (METALIMPHY), France. It is sold by other companies under several other tradenames, e.g. NILVAR. At temperatures above 400C, its thermal expansion coeff. is comparable to other Ni alloys. Ferromagnetic
INVAR Standards with similar compositions(cold worked, hard)