Compositional summary
Fe73-87 / Cr11-14 / C1.8-3.6 / Mn0.15-1.5 (impurities: Mo<3, Cu<2, Ni<2, Si<1, P<0.1, S<0.1)
Material family: Metal (ferrous)
Base material: Fe (Iron)
| Elements | Min | Max | % | ||
|---|---|---|---|---|---|
| C (carbon) | 1.8 | – | 3.6 | % | |
| Cr (chromium) | 11 | – | 14 | % | |
| Cu (copper) | 0 | – | 2 | % | |
| Fe (iron) | 72.8 | – | 87.1 | % | |
| Mn (manganese) | 0.15 | – | 1.5 | % | |
| Mo (molybdenum) | 0 | – | 3 | % | |
| Ni (nickel) | 0 | – | 2 | % | |
| P (phosphorus) | 0 | – | 0.1 | % | |
| S (sulfur) | 0 | – | 0.1 | % | |
| Si (silicon) | 0 | – | 1 | % |