EN GJN HV600 Chemical Composition, former BS 2D, Cast iron, white, Ni-Cr alloy

Compositional summary

Fe76-83 / Cr8-10 / Ni4.5-6.5 / C2.5-3.5 / Si1.5-2.5 / Mn0.2-0.8 (impurities: Mo<0.5, S<0.15, P<0.1)

Material family: Metal (ferrous)

Base material: Fe (Iron)

ElementsMinMax%
C (carbon)2.53.5%
Cr (chromium)810%
Fe (iron)76.183.3%
Mn (manganese)0.20.8%
Mo (molybdenum)00.5%
Ni (nickel)4.56.5%
P (phosphorus)00.1%
S (sulfur)00.15%
Si (silicon)1.52.5%
EN GJN HV600 Chemical Composition, former BS 2D, Cast iron, white, Ni-Cr alloy

Tradenames: NI-HARD TYPE 4, NI-HARD TYPE D, YOONSTEEL N2