Aluminum 6061 Similar Compositions

Designation

6061, wrought
UNS numberA96061
EN name Mg1SiCu)EN AW-6061 (EN AW-Al  
EN number3.3211

Aluminum 6061 Similar Compositions

Australia: 6061 to AS 1734, 6061 to AS 1865, 6061 to AS 1866, 6061 to AS 1867, 6061 to AS 2848.1, 6061A to AS 2848.1
Canada: 0.6061 to CSA HA.4, 0.6061 to CSA HA.5, 0.6061 to CSA HA.6, 0.6061 to CSA HA.7, 0.6061 to CSA HA.7.1, 0.6061 to CSA HA.8
Europe: EN AW-6061 to CEN EN 573-3
France: 6061 to NF A50-411, 6061 to NF A50-451
Germany: 3.3211/AlMgSi1Cu to DIN 1725-1
International: AlMg1SiCu to ISO 209-1
Japan: 6061 to JIS H4120, A6061FD to JIS H4140, A6061FH to JIS H4140, A6061P to JIS H4000, A6061S to JIS H4100, A6061TB to JIS H4180, A6061TD to JIS H4080, A6061TE to JIS H4080
Russia: 1330 to GOST 4784, AD33 to GOST 4784
UK: 6061 to BS 1471, 6061 to BS 1473, 6061 to BS 1474, 6061 to BS 1475
USA: 6061, 6061 to AMS 4025, 6061 to AMS 4026, 6061 to AMS 4027, 6061 to AMS 4043, 6061 to AMS 4053, 6061 to AMS 4115, 6061 to AMS 4116, 6061 to AMS 4117, 6061 to ASTM B209M, 6061 to ASTM B210M, 6061 to ASTM B211M, 6061 to ASTM B221M, 6061 to ASTM B234, 6061 to ASTM B241M, 6061 to ASTM B247M, 6061 to ASTM B308/B308M, 6061 to ASTM B313/B313M, 6061 to ASTM B316/B316M, 6061 to ASTM B345/B345M, 6061 to ASTM B404/B404M, 6061 to ASTM B429, 6061 to ASTM B483/B483M, 6061 to ASTM B547/B547M, 6061 to ASTM B632/B632M, 6061 to MIL F-17132, 6061 to MIL P-25995B, 6061 to QQ A-225/8, 6061 to QQ A-250/11, 6061A, 6062, UNS A96061
Venezuela: 6061 to COPANT 862
Yugoslavia: 3.5456.00/AlMg1SiCu to JUS C.C2.100
Tradenames: ALCOA 6061 COLD FINISHED BAR, ALUMINUM C58, ANTICORODAL-082, BAW 6061, KAISER ALUMINUM 6061

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey