Aluminum 6061 T6 Mechanical Properties
Designation 6061, wrought Condition T6 (Solution heat-treated and artificially aged) UNS number A96061 EN name EN AW-6061 (EN AW-Al Mg1SiCu) EN number 3.3211 Aluminum 6061 T6 Mechanical Properties Young’s modulus 66.6 – 70 GPa Specific stiffness 24.5 – 25.8 MN.m/kg Yield strength (elastic limit) 240 – 280 MPa Tensile strength 290 – 338 MPa Specific … Continue reading Aluminum 6061 T6 Mechanical Properties