Aluminum 6061 T62 Mechanical Properties

Designation
6061, wrought
ConditionT62 (Solution heat-treated and artificially aged)
UNS numberA96061
EN nameEN AW-6061 (EN AW-Al Mg1SiCu)
EN number3.3211

Aluminum 6061 T62 Mechanical Properties

Young’s modulus68–71.5GPa
Specific stiffness25.1–26.4MN.m/kg
Yield strength (elastic limit)241–266MPa
Tensile strength262–296MPa
Specific strength88.8–98.2kN.m/kg
Elongation6–11% strain
Compressive strength234–259MPa
Flexural modulus68–71.5GPa
Flexural strength (modulus of rupture)241–266MPa
Shear modulus26–27.3GPa
Bulk modulus66.9–70.3GPa
Poisson’s ratio0.33–0.343 
Shape factor26   
Hardness – Vickers67–108HV
Elastic stored energy (springs)416–509kJ/m^3
Fatigue strength at 10^7 cycles62–100MPa
Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles60.6–102MPa


MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey