Aluminum 6061 T62 Mechanical Properties

Designation 6061, wrought Condition T62 (Solution heat-treated and artificially aged) UNS number A96061 EN name EN AW-6061 (EN AW-Al Mg1SiCu) EN number 3.3211 Aluminum 6061 T62 Mechanical Properties Young’s modulus 68 – 71.5 GPa Specific stiffness 25.1 – 26.4 MN.m/kg Yield strength (elastic limit) 241 – 266 MPa Tensile strength 262 – 296 MPa Specific … Continue reading Aluminum 6061 T62 Mechanical Properties