Aluminum 6061 T4 Mechanical Properties

Designation 6061, wrought Condition T4 (Solution heat-treated and naturally aged to a substantially stable condition) UNS number A96061 EN name EN AW-6061 (EN AW-Al Mg1SiCu) EN number 3.3211 Aluminum 6061 T4 Mechanical Properties Young’s modulus 66.6 – 70 GPa Specific stiffness 24.5 – 25.8 MN.m/kg Yield strength (elastic limit) 92.6 – 108 MPa Tensile strength … Continue reading Aluminum 6061 T4 Mechanical Properties