Aluminum 6061 Chemical Composition

Designation

6061, wrought
UNS numberA96061
EN name Mg1SiCu)EN AW-6061 (EN AW-Al  
EN number3.3211

Aluminum 6061 Composition Detail

Al (aluminum)95.8–98.6%
Cr (chromium)0.04–0.35%
Cu (copper)0.15–0.4%
Fe (iron)0–0.7%
Mg (magnesium)0.8–1.2%
Mn (manganese)0–0.15%
Si (silicon)0.4–0.8%
Ti (titanium)0–0.15%
Zn (zinc)0–0.25%
Other0–0.15%

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey