| AISI 1095, Carbon steel | Equivalent Grades |
|---|---|
| UNS number | G10950 |
| US name | ASTM 1095, ASME G10950 |
| EN name | ~HS95 |
| Germany number | DIN WNr 1.1275 |
| Germany name | DIN Ck100, DIN 17222(79) Ck101, |
Tradenames of AISI 1095, Carbon steel: ACHORN STANDARD CARBON, AIRCO NO. 85, AQUATOUGH 100, ATLAS REFINED-10, BEST, CARR’S QUALITY RED LABEL, CHANNELER, COPPCO EXTRA, CORINTH, DISSTON NO. 5190, EIS-V3, ELECTREX, FAGERSTA OVERCOAT AXE, FAGERSTA REGULAR, FAGERSTA SPECIAL, FIRTH-BROWN F95C, FORTUNA GSB10, FORTUNA W93, G.W. REGULAR, G.W. SPECIAL, H S C COLD HEADER, H S C REGULAR, JESSOP BLUE LABEL, JESSOP SHEET SPRING, K.E.A. 108, MARREL MO, MCINNES FOLDIER DIE, PAGE HIGH CARBON, PREMIER HC WELD, RED SEAL DIE STEEL, S/100, SAVILLE BEST CAST STEEL, SAVILLE CAST, SAVILLE CAST STEEL WARRANTED, SOLID DRILL, SPRING STEEL, STANDARD, TRU-COR DRILL ROD, TULIPE EXTRA NO. 3, UNA NO. 325, WHELCO STD
| Standards with similar compositions: |
|---|
| ONORM M3110 RC95 (Austria) |
| ONORM M3161 C60 (Austria) |
| EN 10016/4(94) 1.1283 (Europe) |
| EN 10016/4(94) C98D2 (Europe) |
| YB/T 5063(93) T10A (China) |
| SFS 906(73) SFS906 (Finland) |
| AFNOR NFA35553 XC100 (France) |
| AFNOR NFA36102(93) C100RR (France) |
| AFNOR NFA36102(93) C125RR (France) |
| AFNOR NFA36102(93) XC100 (France) |
| AFNOR NFA36102(93) XC125 (France) |
| DIN Ck100 (Germany) |
| DIN WNr 1.1275 (Germany) |
| DIN 17140 D95-2 (Germany) |
| DIN 17222(79) C101E (Germany) |
| DIN 17222(79) Ck101 (Germany) |
| DIN 17222(79) WNr 1.1274 (Germany) |
| IS 1570 C98 (India) |
| IS 1570/2(79) 98C6 (India) |
| IS 1570/2(79) C98 (India) |
| IS 3749 T103 (India) |
| UNI 3545 C100 (Italy) |
| UNI 5598(71) 3CD95 (Italy) |
| UNI 7064(82) C100 (Italy) |
| UNI 8893(86) C100 (Italy) |
| NMX-B-301(86) 1095 (Mexico) |
| AS 1442 K1095 (NSW Australia) |
| AS 1442(92) 1095 (NSW Australia) |
| CSA 95-1/1 C1095 (ON Canada) |
| PNH84028 DS105 (Poland) |
| PNH84028 DS95 (Poland) |
| PNH84028 DS96 (Poland) |
| PNH84028 DW100 (Poland) |
| PNH84028 DW95 (Poland) |
| PNH92602 DS105 (Poland) |
| PNH92602 DS95 (Poland) |
| SIS 141870 1870-02 (Sweden) |
| SS 141870 1870 (Sweden) |
| BS 1449/1(91) 95CS (United Kingdom) |
| BS 1449/1(91) 95HS (United Kingdom) |
| BS 970/1(83) 060A96 (United Kingdom) |
| BS 970/1(83) 060A99 (United Kingdom) |
| BS 970/5(72) 060A96 (United Kingdom) |
| BS DEF STAN 95-1-1 C1095 (United Kingdom) |
| AMS 5121G(90) (USA) |
| AMS 5122G(90) (USA) |
| AMS 5132H(93) (USA) |
| AMS 7304 (USA) |
| AMS 8559(98) (USA) |
| ASTM A108(95) 1095 (USA) |
| ASTM A29/A29M(93) 1095 (USA) |
| ASTM A510(96) 1095 (USA) |
| ASTM A576(95) 1095 (USA) |
| ASTM A682/A682M(98) 1095 (USA) |
| ASTM A684A684M(86) 1095 (USA) |
| ASTM A713(93) 1095 (USA) |
| ASTM A830/A830M(98) 1095 (USA) |
| FED QQ-S-700D(91) C1095 (USA) |
| MIL-S-11713C(88) 3 (USA) |
| MIL-S-16788A(86) C10 (USA) |
| MIL-S-46049C(98) 1095 (USA) |
| MIL-S-7947A(63) 1095 (USA) |
| MIL-S-8559A1(81) 1095 (USA) |
| SAE J1397(92) 1095 (USA) |
| SAE J403(95) 1095 (USA) |
| AISI 1095 (USA) |
| COPANT 330 1095 (Venezuela) |
| COPANT 331 1095 (Venezuela) |
| PZ90 (Yugoslavia) |
• Mexico:
1086 to NMX-B-301, 1095 to NMX-B-301
• Pan America:
1095 to COPANT 330, 1095 to COPANT 331
• UK:
060A96 to BS 970/1
• USA:
1086, 1086 to ASTM A29/A29M, 1086 to ASTM A568/A568M, 1086 to ASTM A713, 1086 to SAE J1249, 1086 to SAE J403, 1095, 1095 to ASTM A29/A29M, 1095 to ASTM A568/A568M, 1095 to ASTM A713, 1095 to MIL-S-7947A, 1095 to SAE J403, 7304 to AMS 7304, C10 to MIL-S-16788A, C1095 to FED QQ-S-700D, G10860 to ASTM A510/A510M, G10950 to ASTM A510/A510M, G10950 to ASTM A576-90b, UNS G10860, UNS G10860 to UNS, UNS G10950, UNS G10950 to UNS
Modulus Metal | Sand Casting | Investment Casting | Foundry | CNC Machining | Press Bending | Plastics Injection Molding | Laser Cutting | Welding | Products | Supplier Company | Manufacturer | Service Provider | Exporter | Modulus Metal in TURKEY | Türkiye