| AISI 1080, Carbon steel | Equivalent Grades |
|---|---|
| UNS number | G10800 |
| US name | ASTM Class C, ASTM 1080, ASME G10800, ~ASTM G10780, ~ASTM 1078 |
| EN name | ~HS80 |
| Germany number | DIN WNr 1.1259 |
| Germany name | DIN 80Mn4, DIN D85-3 |
Tradenames of AISI 1080, Carbon steel: B/82, BOHLER NAB, DISSTON NO. 5390, FIRTH-BROWN F75C, FORTUNA HSB2, FORTUNA W83K, INGERSOLL I-75, INGERSOLL I-85, KRUPP W 93, S/83, SANDVIK 13LM, SODERFORS ANVIL, SPEAR 75, TULIPE EXTRA NO. 4, VEW B908
| Standards with similar compositions: |
|---|
| IAS IRAM 1080 (Argentina) |
| EN 10016/2(94) 1.0622 (Europe) |
| EN 10016/2(94) 1.0626 (Europe) |
| EN 10016/2(94) C80D (Europe) |
| EN 10016/2(94) C82D (Europe) |
| EN 10016/4(94) 1.1255 (Europe) |
| EN 10016/4(94) 1.1262 (Europe) |
| EN 10016/4(94) C80D2 (Europe) |
| EN 10016/4(94) C82D2 (Europe) |
| NBN 253-05 C79 (Belgium) |
| BDS 6742(83) 80 (Bulgaria) |
| GB 699(88) 80 (China) |
| YB/T 5063(93) T8A (China) |
| YB/T 5101(93) 80 (China) |
| YB/T 5103(93) 80 (China) |
| SFS 1265(87) SFS1265 (Finland) |
| AFNOR XC80 (France) |
| DIN 80Mn4 (Germany) |
| DIN D85-3 (Germany) |
| DIN WNr 1.1259 (Germany) |
| MSZ 5736(88) D80 (Hungary) |
| MSZ 5736(88) D80K (Hungary) |
| MSZ 5736(88) D83 (Hungary) |
| MSZ 5736(88) D83K (Hungary) |
| IS 1570 C80 (India) |
| IS 3749 T80Mn65 (India) |
| IS 4454 3 (India) |
| IS 4454 4 (India) |
| UNI 5598(71) 3CD80 (Italy) |
| NMX-B-301(86) 1080 (Mexico) |
| AS 1442 K1082 (NSW Australia) |
| AS 1442(92) 1080 (NSW Australia) |
| PNH84028 DB80 (Poland) |
| PNH84028 DB85 (Poland) |
| PNH84032 75 (Poland) |
| GOST 1050 80 (Russian Federation) |
| GOST 1050(74) 80 (Russian Federation) |
| GOST 14959 80 (Russian Federation) |
| GOST 14959(79) 80 (Russian Federation) |
| UNE 36015(60) C79 (Spain) |
| UNE 36015(60) F.1410 (Spain) |
| SIS 141778 1778-02 (Sweden) |
| SIS 141778 1778-04 (Sweden) |
| BS 970/1(83) 060A83 (United Kingdom) |
| BS 970/1(83) 070A78 (United Kingdom) |
| BS 970/1(83) 080A78 (United Kingdom) |
| BS 970/1(83) 080A83 (United Kingdom) |
| BS 970/1(96) 060A78 (United Kingdom) |
| BS 970/1(96) 060A81 (United Kingdom) |
| AMS 5110G(95) (USA) |
| ASTM A29/A29M(93) 1080 (USA) |
| ASTM A510(96) 1080 (USA) |
| ASTM A576(95) 1080 (USA) |
| ASTM A682/A682M(98) 1080 (USA) |
| ASTM A684A684M(86) 1080 (USA) |
| ASTM A713(93) 1080 (USA) |
| ASTM A830/A830M(98) 1080 (USA) |
| ASTM A911/A911M(92) (USA) |
| DoD-F-24669/1(86) 1080 (USA) |
| FED QQ-S-700D(91) C1080 (USA) |
| FED QQ-W-470B(85) 1080 (USA) |
| MIL-S-16788A(86) C8 (USA) |
| MIL-S-16974E(86) 1080 (USA) |
| SAE J1397(92) 1080 (USA) |
| SAE J403(95) 1080 (USA) |
| AISI 1080 (USA) |
| COPANT 330 1080 (Venezuela) |
| COPANT 331 1080 (Venezuela) |
• India:
75C6 to IS 1570/2/1, 80C6 to IS 1570/2/1, 85C6 to IS 1570/2/1, C75 to IS 1570/2/1, C80 to IS 1570/2/1, C85 to IS 1570/2/1
• Mexico:
1074 to NMX-B-301, 1080 to NMX-B-301, 1084 to NMX-B-301, 1085 to NMX-B-301
• Pan America:
1080 to COPANT 330, 1080 to COPANT 331
• USA:
1074, 1074 to ASTM A29/A29M, 1074 to ASTM A568/A568M, 1074 to ASTM A713, 1074 to SAE J403, 1080, 1080 to ASTM A29/A29M, 1080 to ASTM A568/A568M, 1080 to ASTM A713, 1080 to DoD-F-24669/1, 1080 to FED QQ-W-470B, 1080 to MIL-S-16974E, 1080 to SAE J403, 1084, 1084 to ASTM A29/A29M, 1084 to ASTM A568/A568M, 1084 to ASTM A713, 1084 to SAE J1249, 1084 to SAE J403, 1085, 1085 to ASTM A568/A568M, 1085 to SAE J403, 1090, 1090 to ASTM A568/A568M, 1090 to SAE J403, 1580, 1580 to SAE J403, C1080 to FED QQ-S-700D, C1084 to FED QQ-S-700D, C8 to MIL-S-16788A, G10740 to ASTM A510/A510M, G10800 to ASTM A510/A510M, G10800 to ASTM A576-90b, G10840 to ASTM A510/A510M, G10840 to ASTM A576-90b, G10850 to ASTM A510/A510M, UNS G10740, UNS G10740 to UNS, UNS G10800, UNS G10800 to UNS, UNS G10840, UNS G10840 to UNS, UNS G10850, UNS G10900, UNS G15800