| AISI 4130 Low alloy steel (4100 Series, Cr-Mo Alloyed, 0.30% C ) | Equivalent Grades |
|---|---|
| UNS number | G41300, ~H41300, ~K13047 |
| US name | AMS 6345, AMS 6346, AMS 6348, AMS 6350, AMS 6356, AMS S 6758, AMS 6370, AMS 6371 |
| EN name | 30CrMo4 |
| EN number | 1.7216, 1.7220, 1.7221, 1.7226, 1.7230 |
| UK name | 30CrMo4 to BS EN 10297-1 |
Tradenames of AISI 4130 Low alloy steel (4100 Series, Cr-Mo Alloyed, 0.30% C ): AIRCO 4130, HARDWEAR 500F, KROPP 23, RQ AR-321, RQ AR-340, RQ AR-360, RQ AR-400, RQAR 300/311, VERTOMAR CM30, VL-30
| Standards with similar compositions: |
|---|
| IAS IRAM 4130 (Argentina) |
| EN 10083/1(91)A1(96) 1.7213 (Europe) |
| EN 10083/1(91)A1(96) 1.7218 (Europe) |
| EN 10083/1(91)A1(96) 25CrMo4 (Europe) |
| EN 10083/1(91)A1(96) 25CrMoS4 (Europe) |
| NBN 253-02 25CrMo4 (Belgium) |
| NBN 253-02 34CrMo4 (Belgium) |
| BDS 6354 30ChMA (Bulgaria) |
| BDS 6354 35ChM (Bulgaria) |
| GB 3077(88) 30CrMo (China) |
| GB 3077(88) 30CrMoA (China) |
| GB 6478(86) ML30CrMo (China) |
| GB/T 3078(94) 30CrMo (China) |
| YB/T 5132(93) 30CrMo (China) |
| CSN 415130 15130 (Czech Republic) |
| CSN 415131 15131 (Czech Republic) |
| SFS 457(73) SFS457 (Finland) |
| SFS 459 Co.35Cr1.1Mo0.20 (Finland) |
| AFNOR NFA35552 30CD4 (France) |
| AFNOR NFA35553 25CD4 (France) |
| AFNOR NFA35556(84) 30CD4 (France) |
| AFNOR NFA35557 30CD4 (France) |
| AFNOR NFA35558(83) 25CD4 (France) |
| DIN 1652(90) 25CrMo4 (Germany) |
| DIN 1652(90) WNr 1.7218 (Germany) |
| MSZ 61(85) CMo1 (Hungary) |
| MSZ 61(85) CMo1E (Hungary) |
| MSZ 6251(87) CMo1Z (Hungary) |
| UNI 6403(86) 25CrMo4 (Italy) |
| UNI 6403(86) 30CrMo4 (Italy) |
| UNI 6928(71) 25CrMo4F (Italy) |
| UNI 7356 35CrMo4KB (Italy) |
| UNI 7356(74) 25CrMo4KB (Italy) |
| UNI 7845(78) 25CrMo4 (Italy) |
| UNI 7845(78) 30CrMo4 (Italy) |
| UNI 7874(79) 25CrMo4 (Italy) |
| UNI 7874(79) 30CrMo4 (Italy) |
| UNI 8913(87) 25CrMo4 (Italy) |
| JIS G3311(88) SCM430M (Japan) |
| JIS G3441(88) SCM430TK (Japan) |
| JIS G3441(88) STKS1 (Japan) |
| JIS G3441(88) STKS3 (Japan) |
| JIS G4105(79) SCM 1 (Japan) |
| JIS G4105(79) SCM 2 (Japan) |
| JIS G4105(79) SCM24 (Japan) |
| JIS G4105(79) SCM430 (Japan) |
| JIS G4105(79) SCM432 (Japan) |
| JIS G4105(79) SCM822 (Japan) |
| DGN B-203 4130 (Mexico) |
| DGN B-297 4130 (Mexico) |
| NMX-B-300(91) 4130 (Mexico) |
| AS 1444(96) 4130 (NSW Australia) |
| PNH84030/04 25HM (Poland) |
| PNH84030/04 30HM (Poland) |
| STAS 25MoCr11 (Romania) |
| STAS 11500/2 30MoCr10 (Romania) |
| STAS 11500/2 33MoCr10 (Romania) |
| STAS 11500/2(89) 30MoCr11 (Romania) |
| STAS 791(88) 19MoCr11 (Romania) |
| STAS 791(88) 19MoCr11S (Romania) |
| STAS 791(88) 19MoCr11X (Romania) |
| STAS 791(88) 19MoCr11XS (Romania) |
| STAS 791(88) 26MoCr11 (Romania) |
| STAS 791(88) 26MoCr11S (Romania) |
| STAS 791(88) 26MoCr11X (Romania) |
| STAS 791(88) 26MoCr11XS (Romania) |
| STAS 9382/4 33MoCr11q (Romania) |
| GOST 10702 30ChMA (Russian Federation) |
| GOST 4543 30ChM (Russian Federation) |
| GOST 4543 30ChMA (Russian Federation) |
| GOST 4543(71) 20ChM (Russian Federation) |
| GOST 4543(71) 30ChM (Russian Federation) |
| GOST 4543(71) 30ChMA (Russian Federation) |
| UNE 36012(75) 30CrMo4 (Spain) |
| UNE 36012(75) 30CrMo4-1 (Spain) |
| UNE 36012(75) F.1251 (Spain) |
| UNE 36012(75) F.1256 (Spain) |
| UNE 36034(85) 35CrMo4DF (Spain) |
| SIS 142225 2225-01 (Sweden) |
| SIS 142225 2225-03 (Sweden) |
| SIS 142225 2225-04 (Sweden) |
| SIS 142225 2225-05 (Sweden) |
| SIS 142225 2225-06 (Sweden) |
| SIS 142225 2225-07 (Sweden) |
| SS 142225 2225 (Sweden) |
| SS 142233 2233 (Sweden) |
| ISO 683-2(68) Type 1 (International) |
| ISO 683-4 Type 2a (International) |
| ISO 683-4 Type 2b (International) |
| BS 1717(83) CDS110 (United Kingdom) |
| BS 970/1(83) 708A30 (United Kingdom) |
| AMS 6348 (USA) |
| AMS 6350 (USA) |
| AMS 6351 (USA) |
| AMS 6360 (USA) |
| AMS 6361 (USA) |
| AMS 6362 (USA) |
| AMS 6370 (USA) |
| AMS 6371 (USA) |
| AMS 6373 (USA) |
| AMS 6374 (USA) |
| AMS 6528 (USA) |
| AMS 7496 (USA) |
| ASTM A29/A29M(93) 4130 (USA) |
| ASTM A322(96) 4130 (USA) |
| ASTM A331(95) 4130 (USA) |
| ASTM A372 Grade 1 (USA) |
| ASTM A506(93) 4130 (USA) |
| ASTM A507(93) 4130 (USA) |
| ASTM A513(97a) 4130 (USA) |
| ASTM A519(96) 4130 (USA) |
| ASTM A646(95) Grade 11 (USA) |
| ASTM A752(93) 4130 (USA) |
| ASTM A752(93) 5130 (USA) |
| ASTM A829/A829M(95) 4130 (USA) |
| ASTM A866(94) 4130 (USA) |
| ASTM A983/983M(98) Grade 3 (USA) |
| DoD-F-24669/1(86) 4130 (USA) |
| MIL-S-16974E(86) 4130 (USA) |
| MIL-S-18729C(66) 4130 (USA) |
| MIL-S-46059 G41300 (USA) |
| MIL-S-6758 – – – (USA) |
| MIL-T-6736B – – – (USA) |
| SAE 770(84) 4130 (USA) |
| SAE J404(94) 4130 (USA) |
| AISI 4130 (USA) |
| COPANT 334 4130 (Venezuela) |
| COPANT 514 4130 (Venezuela) |
| C.4730 (Yugoslavia) |
| C.4781 (Yugoslavia) |
• Argentina:
IRAM 4130 to IAS
• Australia:
4130 to AS 1444, 4130H to AS 1444
• Czech Republic:
15131 to CSN 415131
• India:
30Cr4Mo2 to IS 1570/4, IS 963 to IS 963
• Italy:
30CrMo4 to UNI 6403, 30CrMo4 to UNI 7845, 30CrMo4 to UNI 7874
• Japan:
SCM 1 to JIS G4105, STH 21 to JIS G3429, STKS1 to JIS G3441, STKS3 to JIS G3441
• Mexico:
4130 to NMX-B-203-SCFI, 4130 to NMX-B-300, 4130H to NMX-B-268, 4130H to NMX-B-300
• Pan America:
4130 to COPANT 334, 4130 to COPANT 514
• Poland:
30HM to PN-H-84030/04, 30HMA to PN-H-84030/04
• Romania:
25MoCr11 to STAS, 33MoCr11q to STAS 9382/4
• UK:
30CrMo4 to BS EN 10297-1
• USA:
4130, 4130 to ASTM A29/A29M, 4130 to ASTM A331-95, 4130 to ASTM A513, 4130 to ASTM A519, 4130 to ASTM A829/A829M, 4130 to ASTM A866, 4130 to DoD-F-24669/1, 4130 to SAE J404, 4130H to ASTM A331-95, 4130H to SAE J1975, G41300 to ASTM A1031, G41300 to ASTM A506, G41300 to ASTM A507, G41300 to MIL-S-46059, Grade 11 to ASTM A646-95, Grade 3 to ASTM A983/A983M, Grade E Class 55 to ASTM A372/A372M, Grade E Class 65 to ASTM A372/A372M, Grade E Class 70 to ASTM A372/A372M, MIL-T-6736 to MIL-T-6736B, UNS G41300, UNS H41300, UNS K13047, UNS K13147
Modulus Metal | Sand Casting | Investment Casting | Foundry | CNC Machining | Press Bending | Plastics Injection Molding | Laser Cutting | Welding | Products | Supplier Company | Manufacturer | Service Provider | Exporter | Modulus Metal in TURKEY | Türkiye