| AISI 4037 Low alloy steel, 4000 Series (Mo Alloyed) 0.37% C | Equivalent Grades |
|---|---|
| UNS number | G40370 |
| US name | SAE 4037, SAE 4032H, ASTM L7A, ASTM 4042H, ASTM 4037H, ASTM 4037, ASTM 4032H, ASTM 4032, ~SAE 4032 |
| International | 36Mo3E to ISO 4954 |
| UK name | 2/1 to BS 3111/1 |
| Germany name | DIN WNr 1.5412 |
Tradenames of AISI 4037 Low alloy steel, 4000 Series (Mo Alloyed) 0.37% C: SHARON 4000 SERIES, WEST NO. 7 (DURACAST), WEST NO. 7A (DURACAST)
| Standards with similar compositions: |
|---|
| DIN WNr 1.5412 (Germany) |
| IS 5517 35Mn2Mo28 (India) |
| IS G18 EN16 (India) |
| IS G18 EN16D (India) |
| DGN B-203 4037 (Mexico) |
| DGN B-297 4037 (Mexico) |
| NMX-B-300(91) 4037 (Mexico) |
| AS 1444(96) 4037 (NSW Australia) |
| AS G18 En16C (NSW Australia) |
| GOST 21357 35MLS (Russian Federation) |
| UNE F.120.I (Spain) |
| BS 3111/1(87) 01/02/2001 (United Kingdom) |
| BS 3111/1(87) 02/02/2001 (United Kingdom) |
| BS 970/1(83) 605A37 (United Kingdom) |
| BS 970/1(83) 605H37 (United Kingdom) |
| AMS 6300 4037 (USA) |
| ASTM A29/A29M(93) 4037 (USA) |
| ASTM A322(96) 4037 (USA) |
| ASTM A331(95) 4037 (USA) |
| ASTM A519(96) 4037 (USA) |
| ASTM A752(93) 4037 (USA) |
| SAE 770(84) 4037 (USA) |
| SAE J404(94) 4037 (USA) |
| AISI 4037 (USA) |
| COPANT 334 4037 (Venezuela) |
• Australia:
4037 to AS 1444, En16C to AS G18
• International:
36Mo3E to ISO 4954
• Mexico:
4032 to NMX-B-300, 4032H to NMX-B-268, 4032H to NMX-B-300, 4037 to NMX-B-203-SCFI, 4037 to NMX-B-300, 4037H to NMX-B-268, 4037H to NMX-B-300
• Pan America:
4037 to COPANT 334
• Serbia and Montenegro:
C.1436
• UK:
2/1 to BS 3111/1
• USA:
4032, 4032 to ASTM A29/A29M, 4032H to ASTM A331-95, 4037 to ASTM A29/A29M, 4037 to ASTM A331-95, 4037 to ASTM A519, 4037 to SAE J404, 4037 to SAE J770, 4037H to ASTM A331-95, L71 to ASTM A320/A320M, L7A to ASTM A320/A320M, UNS G40320, UNS G40370, UNS H40320, UNS H40370