| AISI 1340, Carbon steel ( Manganese Steel, 0.4% C ) | Equivalent Grades |
|---|---|
| UNS number | G13400, ~H13400 |
| EN name | BS S 156, BS S 157, 38Mn6 |
| EN number | 1.1127 |
| Germany name | 36Mn6 to DIN, 46Mn7 to DIN |
| International name | 36Mn6 to ISO 683-1, 36Mn6 to ISO 683-18, 42Mn6 to ISO 683-1, 42Mn6 to ISO 683-18, 42Mn6E to ISO 4954 |
Tradenames of AISI 1340, Carbon steel ( Manganese Steel, 0.4% C ): A-1203, AR, AR-235 (1), BOHLER V742, COLFORM E.T.D. 1541 A, COLFORM E.T.D. 1541 B, INTERMEDIATE MANGANESE ABRASION STEEL, KAISALOY AR, KRUPP 36 MN 6, KRUPP 46 MN 7, POMPEY 1541, ROC 250, SHEFFIELD-AR, XK1335, XK1340, XK1345
| Standards with similar compositions: |
|---|
| BDS 6354 40G2F (Bulgaria) |
| GB 3077(88) 40Mn2 (China) |
| GB 8162(87) 40Mn2 (China) |
| GB/T 3078(94) 40Mn2 (China) |
| YB/T 5052(93) 40Mn2 (China) |
| DIN 42MnV7 (Germany) |
| DIN WNr 1.5223 (Germany) |
| DGN B-203 1340 (Mexico) |
| DGN B-297 1340 (Mexico) |
| NMX-B-300(91) 1340 (Mexico) |
| AS 1442 K1340 (NSW Australia) |
| AS 1442(92) X1340 (NSW Australia) |
| AS 1443(94) X1340 (NSW Australia) |
| ASTM A29/A29M(93) 1340 (USA) |
| ASTM A322(96) 1340 (USA) |
| ASTM A331(95) 1340 (USA) |
| ASTM A519(96) 1340 (USA) |
| ASTM A547 1340 (USA) |
| ASTM A752(93) 1340 (USA) |
| ASTM A829/A829M(95) 1340 (USA) |
| DoD-F-24669/1(86)(86) 1340 (USA) |
| MIL-S-16974E(86) 1340 (USA) |
| SAE 770(84) 1340 (USA) |
| SAE J404(94) 1340 (USA) |
| AISI 1340 (USA) |
| COPANT 334 1340 (Venezuela) |
| COPANT 514 1340 (Venezuela) |
• Australia:
K1340 to AS 1442, X1340 to AS 1442, X1340 to AS 1443, X1345 to AS 1442
• China:
45Mn2 to GB/T 11251
• France:
40M6 to AFNOR NF A35-552
• Germany:
36Mn6 to DIN, 46Mn7 to DIN
• India:
37C15 to IS 11169/1, 37C15 to IS 13352, 37C15 to IS 9175/15, 37Mn2 to IS 4368
• International:
36Mn6 to ISO 683-1, 36Mn6 to ISO 683-18, 42Mn6 to ISO 683-1, 42Mn6 to ISO 683-18, 42Mn6E to ISO 4954
• Japan:
SMn 2 to JIS G4106, SMn 3 to JIS G4106, SMn2H to JIS G4052, SMn3H to JIS G4052, SWRCH41K to JIS G3507
• Mexico:
1335 to NMX-B-300, 1340 to NMX-B-203-SCFI, 1340 to NMX-B-300, 1340H to NMX-B-300, 1345 to NMX-B-203-SCFI, 1345 to NMX-B-300, 1345H to NMX-B-268, 1345H to NMX-B-300, 1541 to NMX-B-301
• Pan America:
1335 to COPANT 514, 1340 to COPANT 334, 1340 to COPANT 514, 1345 to COPANT 514
• South Korea:
SMn 438 H to KS D 3754, SMn 438 to KS D 3724, SMn 443 H to KS D 3754, SMn 443 to KS D 3724, SWRCH41K to KS D 3592
• USA:
1335, 1335 to ASTM A29/A29M, 1335 to ASTM A331-95, 1335 to ASTM A519, 1335 to ASTM A829/A829M, 1335 to DoD-F-24669/1, 1335 to MIL-S-16974E, 1335 to SAE J404, 1335 to SAE J770, 1340, 1340 to ASTM A29/A29M, 1340 to ASTM A331-95, 1340 to ASTM A513, 1340 to ASTM A519, 1340 to ASTM A829/A829M, 1340 to MIL-S-16974E, 1340 to SAE J404, 1340 to SAE J770, 1345, 1345 to ASTM A29/A29M, 1345 to ASTM A331-95, 1345 to ASTM A519, 1345 to ASTM A829/A829M, 1345 to FED QQ-S-626C, 1345 to SAE J404, 1345 to SAE J770, 1541H, 1541H to ASTM A304, 1541H to SAE J1268, 15B41H, 15B41H to ASTM A304, 15B41H to SAE J1268, 15L41H, E1541H, G15410 to ASTM A830/A830M, H15410 to SAE J775, NV1 to SAE J775, UNS G13350, UNS G13400, UNS G13450, UNS H13350, UNS H13400, UNS H13450, UNS H15410, UNS H15411
Modulus Metal | Sand Casting | Investment Casting | Foundry | CNC Machining | Press Bending | Plastics Injection Molding | Laser Cutting | Welding | Products | Supplier Company | Manufacturer | Service Provider | Exporter | Modulus Metal in TURKEY | Türkiye