| AISI 1060, Carbon steel | Equivalent Grades |
|---|---|
| UNS number | G10600 |
| US name | ASTM Class B, ASTM 1060, ASME G10600, ~ASME G10590, ~ASME 1059 |
| EN name | ~HS60 |
| Germany name | DIN EN 10083(91) CK60 |
| France name | AFNOR NFA35553 XC60 |
Tradenames of AISI 1060, Carbon steel: AGATHON BIT STEEL, AMALOY, B/70, DIE BLOCK (A), FORTUNA GSB63, FORTUNA W63, HI-QUA-LED 10L60, INGERSOLL I-60, KRUPP 1740, MARREL M2, PREMIER MB SPRING, PREMIER SPRING, S/70, SHOCK RESISTING, SIMONDS 1064 RULE DIE, SPRING STEEL SHEET, TULIPE EXTRA NO. 5, VEW Z988
| Standards with similar compositions: |
|---|
| IAS IRAM 1060 (Argentina) |
| ONORM M3161 C60 (Austria) |
| EN 10016/2(94) 1.061 (Europe) |
| EN 10016/2(94) C60D (Europe) |
| EN 10016/4(94) 1.1226 (Europe) |
| EN 10016/4(94) C60D2 (Europe) |
| EN 10083/1(91)A1(96) 1.1221 (Europe) |
| EN 10083/1(91)A1(96) 1.1223 (Europe) |
| EN 10083/1(91)A1(96) C60E (Europe) |
| EN 10083/1(91)A1(96) C60R (Europe) |
| EN 10083/2(91)A1(96) 1.0601 (Europe) |
| EN 10083/2(91)A1(96) C60 (Europe) |
| NBN 253-02 C60-1 (Belgium) |
| NBN 253-02 C60-2 (Belgium) |
| NBN 253-02 C60-3 (Belgium) |
| BDS 5785(83) 60 (Bulgaria) |
| BDS 6742(82) 60G (Bulgaria) |
| GB 3522(83) 60 (China) |
| GB 699(88) 60 (China) |
| GB/T 3078(94) 60 (China) |
| YB/T 5101(93) 60 (China) |
| YB/T 5103(93) 60 (China) |
| CSN 411700 11700 (Czech Republic) |
| CSN 412061 12061 (Czech Republic) |
| AFNOR CC55 (France) |
| AFNOR NFA35553 XC60 (France) |
| DIN 60Mn3 (Germany) |
| DIN WNr 1.0642 (Germany) |
| DIN EN 10083(91) CK60 (Germany) |
| DIN EN 10083(91) Cm60 (Germany) |
| DIN EN 10083(91) WNr 1.0601 (Germany) |
| DIN EN 10083(91) WNr 1.1223 (Germany) |
| MSZ 4217(85) C60 (Hungary) |
| MSZ 61 C60Ek (Hungary) |
| MSZ 61(85) C60 (Hungary) |
| MSZ 61(85) C60E (Hungary) |
| IS 1570 C60 (India) |
| IS 4454 SW (India) |
| UNI 3545 C60 (Italy) |
| UNI 5598(71) 3CD60 (Italy) |
| UNI 7064(82) C60 (Italy) |
| UNI 7065(72) C60 (Italy) |
| UNI 7065(72) C61 (Italy) |
| UNI 7845(78) C60 (Italy) |
| UNI 7874(79) C60 (Italy) |
| UNI 8893(86) C60 (Italy) |
| JIS G3311(88) S60CM (Japan) |
| JIS G3311(88) S65CM (Japan) |
| JIS G4051(79) S58C (Japan) |
| NMX-B-301(86) 1060 (Mexico) |
| AS 1442 K1060 (NSW Australia) |
| AS 1442(92) 1060 (NSW Australia) |
| PNH84019 60 (Poland) |
| PNH84019 60G (Poland) |
| PNH84028 D55 (Poland) |
| STAS 880(88) OLC60 (Romania) |
| STAS 880(88) OLC60S (Romania) |
| STAS 880(88) OLC60X (Romania) |
| STAS 880(88) OLC60XS (Romania) |
| GOST 1050(74) 60G (Russian Federation) |
| GOST 1050(88) 60 (Russian Federation) |
| GOST 10791 2 (Russian Federation) |
| GOST 14959 60G (Russian Federation) |
| GOST 398 II (Russian Federation) |
| GOST 398 III (Russian Federation) |
| GOST 4121 K62 (Russian Federation) |
| GOST 4121 K63 (Russian Federation) |
| SS 141665 1665 (Sweden) |
| SS 141678 1678 (Sweden) |
| ISO 683-1(87) C60 (International) |
| ISO 683-1(87) C60E4 (International) |
| ISO 683-1(87) C60M2 (International) |
| ISO 683-18(96) C60 (International) |
| ISO 683-18(96) C60E4 (International) |
| ISO 683-18(96) C60M2 (International) |
| ISO 683-3(70) C60ea (International) |
| ISO R683-3(70) C60eb (International) |
| VSM 10648 C60 (Switzerland) |
| VSM 10648 CK60 (Switzerland) |
| BS 1449/1(91) 60CS (United Kingdom) |
| BS 1449/1(91) 60HS (United Kingdom) |
| BS 970/1(83) 060A57 (United Kingdom) |
| BS 970/1(83) 080A57 (United Kingdom) |
| BS 970/1(96) 060A62 (United Kingdom) |
| AMS 7240 (USA) |
| ASTM A29/A29M(93) 1060 (USA) |
| ASTM A510(96) 1060 (USA) |
| ASTM A513(97a) 1060 (USA) |
| ASTM A576(95) 1060 (USA) |
| ASTM A682/A682M(98) 1060 (USA) |
| ASTM A684A684M(86) 1060 (USA) |
| ASTM A713(93) 1060 (USA) |
| ASTM A830/A830M(98) 1060 (USA) |
| DoD-F-24669/1(86) 1060 (USA) |
| FED QQ-S-00640(63) 1060 (USA) |
| FED QQ-S-633A(63) 1060 (USA) |
| MIL-S-10520D(AR)(88) 5 (USA) |
| MIL-S-10520D(AR)(88) 7 (USA) |
| MIL-S-16788A(86) C6 (USA) |
| MIL-S-16974E(86) 1060 (USA) |
| SAE J1397(92) 1060 (USA) |
| SAE J403(95) 1060 (USA) |
| AISI 1060 (USA) |
| COPANT 330 1060 (Venezuela) |
| COPANT 331 1060 (Venezuela) |
| COPANT 333 1060 (Venezuela) |
| C.1700 (Yugoslavia) |
| C.1730 (Yugoslavia) |
| C.1731 (Yugoslavia) |
| C.1780 (Yugoslavia) |
• Belgium:
C55-2 to NBN 253-02, C55-3 to NBN 253-02
• India:
2.49 mm to IS 4824, 60C6 to IS 1570/2/1, 65C6 to IS 1570/2/1, C65 to IS 1570/2/1, IS 4824 to IS 4824
• Mexico:
1059 to NMX-B-301, 1060 to NMX-B-301, 1064 to NMX-B-301, 1065 to NMX-B-301, 1561 to NMX-B-301, B366 to NMX-B-366
• Pan America:
1060 to COPANT 330, 1060 to COPANT 331, 1060 to COPANT 333, 1061 to COPANT 333
• USA:
1055, 1055 to ASTM A568/A568M, 1055 to SAE J403, 1059, 1059 to ASTM A29/A29M, 1059 to ASTM A713, 1059 to SAE J1249, 1060, 1060 to ASTM A29/A29M, 1060 to ASTM A513, 1060 to ASTM A568/A568M, 1060 to ASTM A713, 1060 to DoD-F-24669/1, 1060 to FED QQ-S-00640, 1060 to FED QQ-S-633A, 1060 to MIL-S-16974E, 1060 to SAE J403, 1062, 1064, 1064 to ASTM A29/A29M, 1064 to ASTM A568/A568M, 1064 to ASTM A713, 1064 to SAE J1249, 1065, 1065 to ASTM A29/A29M, 1065 to ASTM A568/A568M, 1065 to ASTM A713, 1065 to SAE J403, 1561, 1561 to ASTM A29/A29M, 1561 to ASTM A713, 7240 to AMS 7240, C6 to MIL-S-16788A, G10590 to ASTM A510/A510M, G10600 to ASTM A510/A510M, G10600 to ASTM A576-90b, G10640 to ASTM A510/A510M, G10650 to ASTM A510/A510M, G15610 to ASTM A510/A510M, G15610 to ASTM A576-90b, Type A Class I to ASTM A417-93, Type A Class II to ASTM A417-93, Type A to ASTM A407-93, Type B Class I to ASTM A417-93, Type B Class II to ASTM A417-93, Type B to ASTM A407-93, Type C Class I to ASTM A417-93, Type C to ASTM A407-93, Type D to ASTM A407-93, Type E to ASTM A407-93, Type F to ASTM A407-93, Type G to ASTM A407-93, Type H to ASTM A407-93, UNS G10590, UNS G10600, UNS G10640, UNS G10640 to UNS, UNS G10650, UNS G10650 to UNS, UNS G15610, UNS K06201
Modulus Metal | Sand Casting | Investment Casting | Foundry | CNC Machining | Press Bending | Laser Cutting | Welding | Products | Supplier Company | Manufacturer | Service Provider | Exporter | Modulus Metal in TURKEY | Türkiye