| AISI 1050, Carbon steel | Equivalent Grades |
|---|---|
| UNS number | G10500 |
| US name | ASTM 1050 Class B, ASTM 1050 Class A, ASTM 1050, ASME G10530, ASME G10500, ASME G10490, ~ASME 1053, ~ASME 1049 |
| EN name | ~~HS50, ~Ck53 |
| UK name | 060A52 to BS 970/1, 070M55 to BS 970/1, 080A52 to BS 970/1, 080H46 to BS 970/1, 080M46 to BS 970/1 |
| JIS (Japanese) name | ~STKM17C, ~STKM17A |
Tradenames of AISI 1050, Carbon steel: ASCOMETAL 51S7, ASCOMETAL XC55H1-H2, B.S.C. A-31, B/55, BOHLER WB, CARR’S QUALITY P 256, DYNAMIC C-1-6, HARDFLEX-11, HI-QUA-LED 10L50, INGERSOLL I-50, LASALLE 1045, MARREL M3, RED DIAMOND 9H, SECO XXX, SIMONDS 1050 ROTARY RULE, STRAIN TEMPERED 1050, TULIPE EXTRA NO. 6, WITTEN W 50 E, WYCO 100-50
| Standards with similar compositions: |
|---|
| IAS IRAM 1050 (Argentina) |
| ONORM M3110 RC50 (Austria) |
| EN 10016/2(94) 1.0586 (Europe) |
| EN 10016/2(94) C50D (Europe) |
| EN 10016/4(94) 1.1171 (Europe) |
| EN 10016/4(94) C50D2 (Europe) |
| EN 10083/1(91)A1(96) 1.1206 (Europe) |
| EN 10083/1(91)A1(96) 1.1241 (Europe) |
| EN 10083/1(91)A1(96) C50E (Europe) |
| EN 10083/1(91)A1(96) C50R (Europe) |
| EN 10083/2(91)A1(96) 1.054 (Europe) |
| EN 10083/2(91)A1(96) C50 (Europe) |
| NBN 253-06 C53 (Belgium) |
| BDS 3492(86) 55LI (Bulgaria) |
| BDS 3492(86) 55LII (Bulgaria) |
| BDS 3492(86) 55LIII (Bulgaria) |
| BDS 5785(83) 50 (Bulgaria) |
| GB 13237(91) 50 (China) |
| GB 3275(91) 50 (China) |
| GB 3522(83) 50 (China) |
| GB 699(88) 50 (China) |
| GB 710(91) 50 (China) |
| GB/T 3078(94) 50 (China) |
| CSN 411600 11600 (Czech Republic) |
| CSN 411650 11650 (Czech Republic) |
| CSN 412051 12051 (Czech Republic) |
| AFNOR NFA35553 XC50 (France) |
| AFNOR NFA36102(93) C50RR (France) |
| AFNOR NFA36102(93) XC50 (France) |
| AFNOR NFA36612(82) F70 (France) |
| DIN D53-3 (Germany) |
| DIN 17230(80) Cf54 (Germany) |
| DIN EN 10016(95) WNr 1.0588 (Germany) |
| DIN EN 10083(91) Ck50 (Germany) |
| DIN EN 10083(91) Cm50 (Germany) |
| DIN EN 10083(91) WNr 1.0540 (Germany) |
| DIN EN 10083(91) WNr 1.1206 (Germany) |
| DIN EN 10083(91) WNr 1.1241 (Germany) |
| DIN SEW 085(88) WNr 1.0555 (Germany) |
| MSZ 2752(89) B1V (Hungary) |
| MSZ 2752(89) B5 (Hungary) |
| MSZ 2898/2(80) A55 (Hungary) |
| MSZ 29(86) A52 (Hungary) |
| MSZ 29(86) A55 (Hungary) |
| MSZ 29/2(64) A55 (Hungary) |
| MSZ 3160(87) A55 (Hungary) |
| MSZ 5736(88) D51 (Hungary) |
| MSZ 5736(88) D51K (Hungary) |
| MSZ 61(85) C50 (Hungary) |
| MSZ 61(85) C50E (Hungary) |
| IS 1570/2(79) 50C4 (India) |
| IS 1570/2(79) 50C8 (India) |
| IS 1570/2(79) C50 (India) |
| IS 3749 T50 (India) |
| IS 5517 C50 (India) |
| UNI 5332 C50 (Italy) |
| UNI 5598 ICD50 (Italy) |
| UNI 5598(71) 1CD50 (Italy) |
| UNI 5598(71) 3CD50 (Italy) |
| UNI 6783 Fe70-3 (Italy) |
| UNI 7065(72) C50 (Italy) |
| UNI 7065(72) C51 (Italy) |
| UNI 7845(78) C50 (Italy) |
| UNI 7874(79) C50 (Italy) |
| UNI 8893(86) C50 (Italy) |
| JIS G4051(79) S50C (Japan) |
| JIS G4051(79) S55C (Japan) |
| NMX-B-301(86) 1050 (Mexico) |
| AS 1442 K1050 (NSW Australia) |
| AS 1442 S1050 (NSW Australia) |
| AS 1442(92) 1050 (NSW Australia) |
| AS 1443 K1050 (NSW Australia) |
| AS 1443 S1050 (NSW Australia) |
| AS 1443(94) 1050 (NSW Australia) |
| PNH84023/07 R55 (Poland) |
| PNH84028 D50 (Poland) |
| PNH84028 D50A (Poland) |
| PNH84028 DW52 (Poland) |
| PNH84032 50S (Poland) |
| STAS 880(88) OLC50 (Romania) |
| STAS 880(88) OLC50S (Romania) |
| STAS 880(88) OLC50X (Romania) |
| STAS 880(88) OLC50XS (Romania) |
| GOST KSt7 (Russian Federation) |
| GOST St7 (Russian Federation) |
| GOST 1050 50 (Russian Federation) |
| GOST 1050(88) 50 (Russian Federation) |
| GOST 1050(88) 05kp (Russian Federation) |
| GOST 10543 Np-50G (Russian Federation) |
| GOST 7521 B56 (Russian Federation) |
| GOST 8531 L53 (Russian Federation) |
| SIS 141674 1674-01 (Sweden) |
| SIS 141674 1674-03 (Sweden) |
| SIS 141674 1674-04 (Sweden) |
| SIS 141674 1674-05 (Sweden) |
| SIS 141674 1674-08 (Sweden) |
| SS 141606 1606 (Sweden) |
| ISO 3304(85) R50 (International) |
| ISO 683-1(87) C50 (International) |
| ISO 683-1(87) C50E4 (International) |
| ISO 683-1(87) C50M2 (International) |
| ISO 683-12 4 (International) |
| ISO 683-12(72) 5 (International) |
| ISO 683-18(96) C50 (International) |
| ISO 683-18(96) C50E4 (International) |
| ISO 683-18(96) C50M2 (International) |
| ISO R683-3(70) C50ea (International) |
| ISO R683-3(70) C50eb (International) |
| TS 911(86) UDK669.14.423 (Turkey) |
| BS 1549 50CS (United Kingdom) |
| BS 1549 50HS (United Kingdom) |
| BS 970/1(83) 060A52 (United Kingdom) |
| BS 970/1(83) 080M50 (United Kingdom) |
| BS 970/3(91) 080M50 (United Kingdom) |
| AMS 5085E(97) (USA) |
| ASTM A108(95) 1050 (USA) |
| ASTM A29/A29M(93) 1050 (USA) |
| ASTM A311/A311M(95) 1050 Class A (USA) |
| ASTM A311/A311M(95) 1050 Class B (USA) |
| ASTM A510(96) 1050 (USA) |
| ASTM A513(97a) 1050 (USA) |
| ASTM A519(96) 1050 (USA) |
| ASTM A576(95) 1050 (USA) |
| ASTM A682/A682M(98) 1050 (USA) |
| ASTM A684A684M(86) 1050 (USA) |
| ASTM A827(98) 1050 (USA) |
| ASTM A830/A830M(98) 1050 (USA) |
| ASTM A866(94) 1050 (USA) |
| DoD-F-24669/1(86) 1050 (USA) |
| FED QQ-S-635B(88) C1050 (USA) |
| FED QQ-S-700D(91) C1050 (USA) |
| MIL-S-10520D(AR)(88) 6 (USA) |
| MIL-S-16788A(86) C5 (USA) |
| MIL-S-16974E(86) 1050 (USA) |
| MIL-S-46059 G10500 (USA) |
| SAE J1397(92) 1050 (USA) |
| SAE J403(95) 1050 (USA) |
| AISI 1050 (USA) |
| COPANT 330 1050 (Venezuela) |
| COPANT 331 1050 (Venezuela) |
| COPANT 333 1050 (Venezuela) |
| COPANT 514 1050 (Venezuela) |
| C.0745 (Yugoslavia) |
| C.1600 (Yugoslavia) |
| PZ50 (Yugoslavia) |
• India:
50C8 to IS 1570/2/1, 55C8 to IS 1570/2/1, C55Mn75 to IS 1570/2/1, CDS-5 to IS 3074, T50 to IS 3749
• Mexico:
1045 to NMX-B-203-SCFI, 1045 to NMX-B-301, 1046 to NMX-B-301, 1049 to NMX-B-301, 1050 to NMX-B-203-SCFI, 1050 to NMX-B-301, 1053 to NMX-B-301, 1055 to NMX-B-301
• Pan America:
1045 to COPANT 330, 1045 to COPANT 331, 1045 to COPANT 333, 1050 to COPANT 330, 1050 to COPANT 331, 1050 to COPANT 333, 1055 to COPANT 330, 1055 to COPANT 331, 1055 to COPANT 333
• UK:
060A52 to BS 970/1, 070M55 to BS 970/1, 080A52 to BS 970/1, 080H46 to BS 970/1, 080M46 to BS 970/1
• USA:
1045, 1045 Class A to ASTM A311/A311M, 1045 Class B to ASTM A311/A311M, 1045 to ASTM A29/A29M, 1045 to ASTM A519, 1045 to ASTM A568/A568M, 1045 to FED QQ-S-700D, 1045 to FED QQ-W-461H, 1045 to SAE J403, 1046, 1046 to ASTM A29/A29M, 1046 to SAE J403, 1049, 1049 to ASTM A29/A29M, 1049 to ASTM A568/A568M, 1049 to SAE J403, 1050, 1050 Class A to ASTM A311/A311M, 1050 Class B to ASTM A311/A311M, 1050 to ASTM A29/A29M, 1050 to ASTM A513, 1050 to ASTM A519, 1050 to ASTM A568/A568M, 1050 to DoD-F-24669/1, 1050 to MIL-S-16974E, 1050 to SAE J403, 1053, 1053 to ASTM A29/A29M, 1053 to SAE J403, 1055, 1055 to ASTM A29/A29M, 1055 to ASTM A713, 1055 to SAE J403, 10L45, 10L50, 1553, C1045 to FED QQ-S-635B, C1050 to FED QQ-S-635B, C1050 to FED QQ-S-700D, C1055 to FED QQ-S-700D, C5 to MIL-S-16788A, G10450 to ASTM A510/A510M, G10450 to ASTM A576-90b, G10460 to ASTM A510/A510M, G10460 to ASTM A576-90b, G10490 to ASTM A510/A510M, G10490 to ASTM A576-90b, G10500 to ASTM A510/A510M, G10500 to ASTM A576-90b, G10500 to MIL-S-46059, G10530 to ASTM A510/A510M, G10530 to ASTM A576-90b, G10550 to ASTM A510/A510M, G10550 to ASTM A576-90b, UNS G10450, UNS G10450 to UNS, UNS G10460, UNS G10490, UNS G10500, UNS G10530, UNS G10550, UNS G15530, UNS K04700
Modulus Metal | Sand Casting | Investment Casting | Foundry | CNC Machining | Press Bending | Laser Cutting | Welding | Products | Supplier Company | Modulus Metal in TURKEY | Türkiye