AISI 1020 steel (UNS G10200) is a low carbon steel. This page lists the AISI 1020 material data sheets for 3 conditions: annealed, as rolled, normalized. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.
Typical Uses of AISI 1020 Steel
Forgings, machined parts, shafts, car wheel hubs, general haulage gear
Looking for AISI 1020 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1020 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low carbon steel grades.