PARA 30% Carbon Fiber (Polyarylamide) Material Data Sheet
PARA 30% Carbon Fiber Overview
PARA 30% carbon fiber is a grade of polyarylamide (PARA), designated Polyarylamide (30% carbon fiber). This PARA 30% carbon fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PARA parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PARA parts in-house and inspects them before shipment.
PARA 30% Carbon Fiber Designation
Polyarylamide (30% carbon fiber)
Tradenames
Ixef, Reny
PARA 30% Carbon Fiber Composition detail
Polymer
70
%
Carbon (fiber)
30
%
PARA 30% Carbon Fiber Physical properties
Density
1.33
–
1.36
g/cm3
PARA 30% Carbon Fiber Mechanical properties
Young’s modulus
22.5
–
28.1
GPa
Specific stiffness
16.7
–
20.9
MN.m/kg
Yield strength (elastic limit)
188
–
235
MPa
Tensile strength
197
–
241
MPa
Specific strength
140
–
175
kN.m/kg
Elongation
1.04
–
1.5
% strain
Elongation at yield
0.879
–
1.67
% strain
Compressive modulus
24.1
–
26.6
GPa
Compressive strength
250
–
276
MPa
Flexural modulus
20.2
–
24.2
GPa
Flexural strength (modulus of rupture)
297
–
363
MPa
Shear modulus
9.33
–
9.81
GPa
Shear strength
118
–
145
MPa
Bulk modulus
22.7
–
25
GPa
Poisson’s ratio
0.321
–
0.323
Shape factor
9.27
Hardness – Vickers
60
–
67
HV
Hardness – Rockwell M
184
–
204
Hardness – Rockwell R
184
–
204
Hardness – Shore D
98
–
102
Elastic stored energy (springs)
695
–
1110
kJ/m3
Fatigue strength at 10^7 cycles
83.3
–
92.1
MPa
PARA 30% Carbon Fiber Impact & fracture properties
Fracture toughness
5.88
–
6.49
MPa.m0.5
Toughness (G)
1.31
–
1.75
kJ/m2
Impact strength, notched 23 °C
3.38
–
6.55
kJ/m2
Impact strength, unnotched 23 °C
43
–
47
kJ/m2
PARA 30% Carbon Fiber Thermal properties
Melting point
269
–
291
°C
Glass temperature
78
–
92.2
°C
Heat deflection temperature 0.45MPa
247
–
268
°C
Heat deflection temperature 1.8MPa
220
–
240
°C
Vicat softening point
77
–
90
°C
Maximum service temperature
188
–
207
°C
Thermal conductivity
0.632
–
0.648
W/m.°C
Specific heat capacity
1480
–
1510
J/kg.°C
PARA 30% Carbon Fiber Electrical properties
Electrical resistivity
2e20
–
5e21
µohm.cm
Electrical conductivity
3.45e-20
–
8.62e-19
%IACS
Dielectric constant (relative permittivity)
3.45
–
5.95
Dissipation factor (dielectric loss tangent)
0.018
–
0.075
Dielectric strength (dielectric breakdown)
15.7
–
17.3
MV/m
Galvanic potential
0.14
–
0.22
V
PARA 30% Carbon Fiber Magnetic properties
Magnetic type
Non-magnetic
PARA 30% Carbon Fiber Optical, aesthetic and acoustic properties