Home » PA (Polyamide / Nylon) » PARA (Polyarylamide) » PARA Unfilled Grades » PARA Unfilled Grade Material Data Sheet
PARA Unfilled Grade (Polyarylamide) Material Data Sheet
PARA Unfilled Grade Overview
PARA unfilled grade is a grade of polyarylamide (PARA), designated Polyarylamide. This PARA unfilled grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PARA parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PARA parts in-house and inspects them before shipment.
PARA Unfilled Grade Designation
Polyarylamide Tradenames Ixef, Nylon-MXD6
PARA Unfilled Grade Typical uses
Automotive, blow molding applications, films (bi-axially oriented, cast, mulatilayer), food applications, monofilaments, packaging, piping, sheet, tubing
PARA Unfilled Grade Composition detail
PARA Unfilled Grade Physical properties
PARA Unfilled Grade Mechanical properties
Young’s modulus 4.4 – 4.7 GPa Specific stiffness 3.69 – 4.1 MN.m/kg Yield strength (elastic limit) 69.4 – 83.9 MPa Tensile strength 83 – 99 MPa Specific strength 58.9 – 72.4 kN.m/kg Elongation 2 – 2.3 % strain Elongation at yield 2.82 – 4.06 % strain Compressive modulus 4.33 – 4.77 GPa Compressive strength 98.9 – 120 MPa Flexural modulus 4.4 – 4.5 GPa Flexural strength (modulus of rupture) 157 – 160 MPa Shear modulus 1.57 – 1.74 GPa Shear strength 49.4 – 59.8 MPa Bulk modulus 4.33 – 4.77 GPa Poisson’s ratio 0.368 – 0.383 Shape factor 5.9 Hardness – Vickers 21 – 24 HV Hardness – Rockwell M 107 – 108 Hardness – Rockwell R 120 – 140 Hardness – Shore D 79 – 92 Elastic stored energy (springs) 533 – 769 kJ/m3 Fatigue strength at 10^7 cycles 33 – 39.9 MPa
PARA Unfilled Grade Impact & fracture properties
Fracture toughness 4.22 – 5.11 MPa.m0.5 Toughness (G) 3.94 – 5.71 kJ/m2 Impact strength, notched 23 °C 1.9 – 2 kJ/m2
PARA Unfilled Grade Thermal properties
Melting point 229 – 245 °C Glass temperature 75 – 92 °C Heat deflection temperature 0.45MPa 145 – 151 °C Heat deflection temperature 1.8MPa 82 °C Maximum service temperature 230 – 239 °C Minimum service temperature -25 °C Thermal conductivity 0.43 – 0.47 W/m.°C Specific heat capacity 1560 – 1630 J/kg.°C Thermal expansion coefficient 50 – 72 µstrain/°C Thermal shock resistance 228 – 343 °C Thermal distortion resistance 0.00622 – 0.00903 MW/m
PARA Unfilled Grade Electrical properties
Electrical resistivity 2e20 – 5e21 µohm.cm Electrical conductivity 3.45e-20 – 8.62e-19 %IACS Dielectric constant (relative permittivity) 3.5
PARA Unfilled Grade Magnetic properties
Magnetic type Non-magnetic
PARA Unfilled Grade Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 1920 – 2029 m/s Mechanical loss coefficient (tan delta) 0.0103 – 0.0149
PARA Unfilled Grade Absorption & permeability
Water absorption @ 24 hrs 0.31 – 5.8 % Water absorption @ sat 5.8 %
PARA Unfilled Grade Processing properties
Polymer injection molding Limited use Polymer extrusion Acceptable Polymer thermoforming Limited use
PARA Unfilled Grade Durability
Water (fresh) Excellent Water (salt) Acceptable Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Limited use Organic solvents Limited use Oils and fuels Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Good Flammability Slow-burning
PARA Grades
PARA Unfilled Material Data Sheets
Unfilled Unfilled You are here
All PARA Grades
Modulus Metal Services
Manufacturing & Quality Services in Turkey