ADI 1400 Austempered Ductile Cast Iron Mechanical Properties

ADI 1400 Mechanical properties

Young’s modulus156–165GPa
Specific stiffness22–23.4MN.m/kg
Yield strength (elastic limit)1030–1240MPa
Tensile strength1400–1550MPa
Specific strength146–175kN.m/kg
Elongation1–3% strain
Compressive modulus156–165GPa
Compressive strength2030–2350MPa
Flexural modulus156–165GPa
Flexural strength (modulus of rupture)1200–1330MPa
Shear modulus57.4–67.8GPa
Shear strength1270–1500MPa
Bulk modulus102–108GPa
Poisson’s ratio0.24–0.25 
Shape factor2.01   
Hardness – Vickers405–450HV
Hardness – Brinell405–450HB
Elastic stored energy (springs)3330–4760kJ/m^3
Fatigue strength at 10^7 cycles435–508MPa

ADI 1400 Impact & fracture properties

Fracture toughness 47–57MPa.m^0.5
Toughness (G) 13.9–20.1kJ/m^2

ADI 1400 Designation

ADI 1400
Condition                                                                                              Cast and austempered

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey