AISI 12L14 Mechanical Properties, Carbon steel, as rolled

AISI 12L14 Mechanical Properties

Young’s modulus196–204GPa
Specific stiffness24.9–25.9MN.m/kg
Yield strength (elastic limit)342–517MPa
Tensile strength380–570MPa
Specific strength43.5–65.7kN.m/kg
Elongation10–17% strain
Compressive strength342–517MPa
Flexural modulus196–204GPa
Flexural strength (modulus of rupture)276–322MPa
Shear modulus77.7–82.4GPa
Bulk modulus152–168GPa
Poisson’s ratio0.29   
Shape factor52   
Hardness – Vickers115–250HV
Hardness – Rockwell B68–84HRB
Hardness – Brinell121–174HB
Elastic stored energy (springs)303–645kJ/m^3
Fatigue strength at 10^7 cycles171–199MPa
Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles126–269MPa

Designation

AISI 12L14
ConditionAs rolled
UNS numberG12144
US nameAISI 12L14, 12L13, 12L15 to ASTM A29, ASTM A510, ASTM A519, ASTM A576, SAE J403
EN name11SMnPb37, 11SMnPb30, 9SMnPb28 to BS EN 10087, BS EN 10277;  S300Pb to NF A35 561
EN number1.0737, 1.0718, 1.9718
JIS (Japanese) nameSUM24L to JIS G4804

AISI 12L14 Impact & fracture properties

Fracture toughness76–92MPa.m^0.5
Toughness (G)29.1–42kJ/m^2


MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey