AISI 3140 Annealed Material Data Sheet

AISI 3140 Annealed Material Data Sheet

AISI 3140 Annealed Overview

AISI 3140 annealed is AISI 3140 low alloy steel (UNS G31400, EN 40NiCr6) in the annealed condition. This AISI 3140 annealed material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Compare all AISI 3140 conditions in our AISI 3140 yield, tensile and hardness comparison. Looking for AISI 3140 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 3140 steel parts in-house and inspects them before shipment.

AISI 3140 Annealed Designation

AISI 3140
ConditionAnnealed
UNS numberG31400
US nameASTM A519
EN name40NiCr6, BS S148, 640M40, EN111
EN number1.5711, 1.5710

AISI 3140 Annealed Typical uses

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 3140 Annealed Composition detail

C (carbon)0.38–0.43%
Cr (chromium)0.55–0.75%
Fe (iron)96.1–97.1%
Mn (manganese)0.7–0.9%
Ni (nickel)1.1–1.4%
P (phosphorus)0–0.04%
S (sulfur)0–0.04%
Si (silicon)0.15–0.35%

AISI 3140 Annealed Physical properties

Density7.8–7.9g/cm3

AISI 3140 Annealed Mechanical properties

Young’s modulus201–212GPa
Specific stiffness25.6–27MN.m/kg
Yield strength (elastic limit)380–470MPa
Tensile strength620–760MPa
Specific strength48.4–59.9kN.m/kg
Elongation19.5–29.5% strain
Compressive strength380–470MPa
Flexural modulus201–212GPa
Flexural strength (modulus of rupture)380–470MPa
Shear modulus77–83GPa
Bulk modulus155–173GPa
Poisson’s ratio0.285–0.295 
Shape factor52
Hardness – Vickers185–225HV
Elastic stored energy (springs)353–530kJ/m3
Fatigue strength at 10^7 cycles306–354MPa
Fatigue strength model (stress range)
Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
267–406MPa

AISI 3140 Annealed Impact & fracture properties

Fracture toughness77–123MPa.m0.5
Toughness (G)30–70.1kJ/m2

AISI 3140 Annealed Thermal properties

Melting point1430–1500°C
Maximum service temperature613–650°C
Minimum service temperature-73–-48°C
Thermal conductivity45–55W/m.°C
Specific heat capacity440–520J/kg.°C
Thermal expansion coefficient10.5–12µstrain/°C
Thermal shock resistance161–207°C
Thermal distortion resistance3.94–4.99MW/m
Latent heat of fusion265–280kJ/kg

AISI 3140 Annealed Electrical properties

Electrical resistivity15–25µohm.cm
Electrical conductivity6.9–11.5%IACS
Galvanic potential-0.5–-0.42V

AISI 3140 Annealed Magnetic properties

Magnetic typeMagnetic

AISI 3140 Annealed Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity5060–5200m/s
Mechanical loss coefficient (tan delta)7e-4–8.7e-4 

AISI 3140 Annealed Processing properties

Metal castingUnsuitable
Metal cold formingExcellent
Metal hot formingExcellent
Metal press formingExcellent
Metal deep drawingLimited use
Machining speed24.4 m/min
Weldability
Notes: Preheating is required, post weld heat treatment may be required
Good
Carbon equivalency0.68 – 0.823

AISI 3140 Annealed Durability

Water (fresh)Acceptable
Water (salt)Limited use
Weak acidsLimited use
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisLimited use
Organic solventsExcellent
Oxidation at 500CAcceptable
UV radiation (sunlight)Excellent
Galling resistance (adhesive wear)Acceptable
FlammabilityNon-flammable

AISI 3140 Annealed Corrosion resistance

Stress corrosion cracking
Note: Rated in chloride; May be susceptible in halide, ammonia, nitrogen, acidic, caustic, carbonate environments
Slightly susceptible

AISI 3140 Annealed Standards with similar compositions

China: 40CrNi to GB/T 17107, 40CrNi to GB/T 3077, 40CrNi to GB/T 3078
India: 35Ni1Cr60 to IS 4368, 35Ni5Cr2 to IS 11169/1, 35Ni5Cr2 to IS 13352, 35Ni5Cr2 to IS 1570/4, 35Ni5Cr2 to IS 3930, 35Ni5Cr2 to IS 4367, 35Ni5Cr2 to IS 9175/24, 46Ni5Cr2 to IS 3445
Japan: SNC 236 to JIS G4053
Romania: 40CrNi12 to STAS 791, 40CrNi12S to STAS 791, 40CrNi12X to STAS 791, 40CrNi12XS to STAS 791, 41CrNi12 to STAS 791
Russia: 40KHN to GOST 4543, 45KHN to GOST 4543, 45KHN to GOST 8479
South Korea: SNC 236 to KS D 3708
USA: 3135, 3140, 3140 to ASTM A519, 3145, G31400 to SAE J775, NV4 to SAE J775, UNS G31400, UNS K22033, X3140
Tradenames: HOFORS KN-14, KRUPP 40 NICR 6