Low Alloy Steel Overview

Low alloy steels are carbon steels with small, deliberate additions of chromium, molybdenum, nickel, vanadium, silicon or boron, usually totalling less than about 5%. These additions raise hardenability, strength and toughness compared with plain carbon steel, so parts can be through-hardened by quenching and tempering in larger sections. Low alloy steels are the workhorse materials for shafts, gears, axles, bolts, crankshafts, springs and high-strength structural and aerospace components.

AISI and SAE Low Alloy Steel Numbering

In the AISI/SAE four-digit system the first two digits identify the main alloying elements and the last two give the nominal carbon content in hundredths of a percent. For example, 41xx steels are chromium-molybdenum steels and AISI 4140 contains about 0.40% carbon; 43xx and 86xx are nickel-chromium-molybdenum steels, 51xx are chromium steels and 92xx are silicon-manganese spring steels. A letter B in the middle, as in 50B46 or 94B30, shows that a small boron addition is used to increase hardenability.

Low Alloy Steel Heat Treatment Conditions

The same low alloy steel can have very different properties depending on its heat treatment. Annealed material is softest and easiest to machine. Normalizing gives a finer, more uniform structure with higher strength. Quenching and tempering produces the highest strength: tempering at a low temperature such as 205°C keeps hardness and tensile strength very high, while tempering at 540–650°C lowers strength but greatly improves toughness and ductility. Each grade below has separate data sheets for each condition, and a comparison post shows how yield strength, tensile strength and hardness change between them.

Low Alloy Steel Parts from Turkey

Looking for low alloy steel parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined low alloy steel parts in-house, including AISI 4140, 4340 and 8620, supplies them heat treated to the required condition, and inspects them before shipment.

Low Alloy Steel Grades and Data Sheets

Molybdenum steels (40xx)

AISI 4037 Low Alloy Steel

AISI 4042 Low Alloy Steel

Chromium-molybdenum steels (41xx)

AISI 4130 Low Alloy Steel

AISI 4135 Low Alloy Steel

AISI 4140 Low Alloy Steel

AISI 4150 Low Alloy Steel

Nickel-chromium-molybdenum steels (43xx, 47xx, 86xx, 87xx, 94xx)

AISI 4320 Low Alloy Steel

AISI 4340 Low Alloy Steel

AISI 8620 Low Alloy Steel

AISI 8630 Low Alloy Steel

AISI 8640 Low Alloy Steel

AISI 8650 Low Alloy Steel

AISI 8660 Low Alloy Steel

AISI 8735 Low Alloy Steel

AISI 8740 Low Alloy Steel

Nickel and nickel-molybdenum steels (31xx, 46xx, 48xx)

AISI 3140 Low Alloy Steel

AISI 4620 Low Alloy Steel

AISI 4820 Low Alloy Steel

Chromium steels (50xx, 51xx)

AISI 5046 Low Alloy Steel

AISI 5130 Low Alloy Steel

AISI 5140 Low Alloy Steel

AISI 5150 Low Alloy Steel

AISI 5160 Low Alloy Steel

Chromium-vanadium steels (61xx)

AISI 6150 Low Alloy Steel

Boron steels (xxBxx)

AISI 50B46 Low Alloy Steel

AISI 50B60 Low Alloy Steel

AISI 51B60 Low Alloy Steel

AISI 81B45 Low Alloy Steel

AISI 86B45 Low Alloy Steel

AISI 94B30 Low Alloy Steel

Silicon-manganese steels (92xx)

AISI 9255 Low Alloy Steel

AISI 9260 Low Alloy Steel

Nickel-chromium-molybdenum steel (93xx)

AISI 9310 Low Alloy Steel

Ultra-high strength steels (300M, 4330V, 4335V, D6AC)

300M Low Alloy Steel

4330V Low Alloy Steel

4335V Low Alloy Steel

D6AC Low Alloy Steel