AISI 4130 Water Quenched & Tempered at 650°C Material Data Sheet

AISI 4130 Water Quenched & Tempered at 650°C Material Data Sheet

AISI 4130 Water Quenched & Tempered at 650°C Overview

AISI 4130 tempered 650°C is AISI 4130 low alloy steel (UNS G41300, EN 30CrMo4) in the water quenched & tempered at 650°C condition. This AISI 4130 tempered 650°C material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Compare all AISI 4130 conditions in our AISI 4130 yield, tensile and hardness comparison. Looking for AISI 4130 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 4130 steel parts in-house and inspects them before shipment.

AISI 4130 Water Quenched & Tempered at 650°C Designation

AISI 4130
ConditionTempered at 650°C & water quenched
UNS numberG41300, ~H41300, ~K13047
US nameAMS 6345, AMS 6346, AMS 6348, AMS 6350, AMS 6356, AMS S 6758, AMS 6370, AMS 6371
EN name30CrMo4
EN number1.7216, 1.7220, 1.7221, 1.7226, 1.7230

AISI 4130 Water Quenched & Tempered at 650°C Typical uses

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 4130 Water Quenched & Tempered at 650°C Composition detail

C (carbon)0.28–0.33%
Cr (chromium)0.8–1.1%
Fe (iron)97.3–98.2%
Mn (manganese)0.4–0.6%
Mo (molybdenum)0.15–0.25%
P (phosphorus)0–0.035%
S (sulfur)0–0.04%
Si (silicon)0.15–0.35%

AISI 4130 Water Quenched & Tempered at 650°C Physical properties

Density7.8–7.9g/cm3

AISI 4130 Water Quenched & Tempered at 650°C Mechanical properties

Young’s modulus201–216GPa
Specific stiffness25.6–27.5MN.m/kg
Yield strength (elastic limit)630–775MPa
Tensile strength730–895MPa
Specific strength80.2–98.7kN.m/kg
Elongation17–27% strain
Compressive strength630–775MPa
Flexural modulus201–216GPa
Flexural strength (modulus of rupture)630–775MPa
Shear modulus77–85GPa
Bulk modulus155–176GPa
Poisson’s ratio0.285–0.295 
Shape factor36
Hardness – Vickers225–275HV
Hardness – Brinell179–270HB
Elastic stored energy (springs)959–1430kJ/m3
Fatigue strength at 10^7 cycles343–397MPa
Fatigue strength model (stress range)
Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
299–456MPa

AISI 4130 Water Quenched & Tempered at 650°C Impact & fracture properties

Fracture toughness48–79MPa.m0.5
Toughness (G)11.6–28.5kJ/m2

AISI 4130 Water Quenched & Tempered at 650°C Thermal properties

Melting point1460–1510°C
Maximum service temperature610–640°C
Minimum service temperature-68–-43°C
Thermal conductivity42–48W/m.°C
Specific heat capacity460–500J/kg.°C
Thermal expansion coefficient11–13µstrain/°C
Thermal shock resistance245–321°C
Thermal distortion resistance3.38–4.17MW/m
Latent heat of fusion265–280kJ/kg

AISI 4130 Water Quenched & Tempered at 650°C Electrical properties

Electrical resistivity20–25µohm.cm
Electrical conductivity6.9–8.62%IACS
Galvanic potential-0.5–-0.42V

AISI 4130 Water Quenched & Tempered at 650°C Magnetic properties

Magnetic typeMagnetic

AISI 4130 Water Quenched & Tempered at 650°C Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity5060–5250m/s
Mechanical loss coefficient (tan delta)5e-4–6.2e-4 

AISI 4130 Water Quenched & Tempered at 650°C Processing properties

Metal castingUnsuitable
Metal cold formingExcellent
Metal hot formingExcellent
Metal press formingExcellent
Metal deep drawingLimited use
Machining speed19.2 m/min
Weldability
Notes: Preheating and post weld heat treatments are required
Good
Carbon equivalency0.537 – 0.7

AISI 4130 Water Quenched & Tempered at 650°C Durability

Water (fresh)Acceptable
Water (salt)Limited use
Weak acidsLimited use
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisLimited use
Organic solventsExcellent
Oxidation at 500CAcceptable
UV radiation (sunlight)Excellent
Galling resistance (adhesive wear)Acceptable
FlammabilityNon-flammable

AISI 4130 Water Quenched & Tempered at 650°C Corrosion resistance

Stress corrosion cracking
Note: Rated in chloride; May be susceptible in halide, ammonia, nitrogen, acidic, caustic, carbonate environments
Slightly susceptible

AISI 4130 Water Quenched & Tempered at 650°C Standards with similar compositions

Argentina: IRAM 4130 to IAS
Australia: 4130 to AS 1444, 4130H to AS 1444
Czech Republic: 15131 to CSN 415131
India: 30Cr4Mo2 to IS 1570/4, IS 963 to IS 963
Italy: 30CrMo4 to UNI 6403, 30CrMo4 to UNI 7845, 30CrMo4 to UNI 7874
Japan: SCM 1 to JIS G4105, STH 21 to JIS G3429, STKS1 to JIS G3441, STKS3 to JIS G3441
Mexico: 4130 to NMX-B-203-SCFI, 4130 to NMX-B-300, 4130H to NMX-B-268, 4130H to NMX-B-300
Pan America: 4130 to COPANT 334, 4130 to COPANT 514
Poland: 30HM to PN-H-84030/04, 30HMA to PN-H-84030/04
Romania: 25MoCr11 to STAS, 33MoCr11q to STAS 9382/4
UK: 30CrMo4 to BS EN 10297-1
USA: 4130, 4130 to ASTM A29/A29M, 4130 to ASTM A331-95, 4130 to ASTM A513, 4130 to ASTM A519, 4130 to ASTM A829/A829M, 4130 to ASTM A866, 4130 to DoD-F-24669/1, 4130 to SAE J404, 4130H to ASTM A331-95, 4130H to SAE J1975, G41300 to ASTM A1031, G41300 to ASTM A506, G41300 to ASTM A507, G41300 to MIL-S-46059, Grade 11 to ASTM A646-95, Grade 3 to ASTM A983/A983M, Grade E Class 55 to ASTM A372/A372M, Grade E Class 65 to ASTM A372/A372M, Grade E Class 70 to ASTM A372/A372M, MIL-T-6736 to MIL-T-6736B, UNS G41300, UNS H41300, UNS K13047, UNS K13147
Tradenames: AIRCO 4130, HARDWEAR 500F, KROPP 23, RQ AR-321, RQ AR-340, RQ AR-360, RQ AR-400, RQAR 300/311, VERTOMAR CM30, VL-30