How do the AISI 3140 heat treatment properties change from one condition to another? This comparison puts the yield strength, tensile strength and hardness of AISI 3140 (UNS G31400, EN 40NiCr6) side by side for 2 conditions: Annealed, Normalized. All values are taken from the individual AISI 3140 material data sheets linked below.
AISI 3140 Yield, Tensile and Hardness by Condition
| Condition | Yield strength (MPa) | Tensile strength (MPa) | Hardness (HV) | Elongation (%) |
|---|---|---|---|---|
| Annealed | 380–470 | 620–760 | 185–225 | 19.5–29.5 |
| Normalized | 540–660 | 800–985 | 240–290 | 16–24 |
AISI 3140 Differences Compared with Annealed
The table below shows how much each condition differs from the annealed condition, based on the mid-point of each range. Positive values mean higher strength or hardness.
| Condition | Yield strength | Tensile strength | Hardness | Elongation |
|---|---|---|---|---|
| Normalized | +41% | +29% | +29% | -18% |
AISI 3140 Strength and Hardness Charts
AISI 3140 Heat Treatment Key Points
The highest tensile strength is reached in the normalized condition (800–985 MPa). The softest condition is annealed (185–225 HV), which is usually preferred for machining and forming.
AISI 3140 Material Data Sheets
AISI 3140 Annealed | AISI 3140 Normalized | All AISI 3140 conditions
Looking for AISI 3140 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 3140 steel parts in-house, heat treated to the condition you specify, and inspects them before shipment.