AISI 9310 Low Alloy Steel

AISI 9310 Low Alloy Steel

AISI 9310 Steel Overview

AISI 9310 steel (UNS G93100, EN 14NiCrMo13-4) is a low alloy steel. This page lists the AISI 9310 material data sheets for 2 conditions: annealed, normalized. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 9310 Steel

Heavy duty aircraft, vehicle transmission gears, track rod pins, roller bearing rings, small arms parts

AISI 9310 Steel Chemical Composition

C (carbon)0.08 – 0.13 %
Cr (chromium)1 – 1.4 %
Fe (iron)93.8 – 95.2 %
Mn (manganese)0.45 – 0.65 %
Mo (molybdenum)0.08 – 0.15 %
Ni (nickel)3 – 3.5 %
P (phosphorus)0 – 0.025 %
S (sulfur)0 – 0.025 %
Si (silicon)0.15 – 0.35 %

AISI 9310 Steel Material Data Sheets

AISI 9310 Annealed Material Data Sheet

AISI 9310 Normalized Material Data Sheet

AISI 9310 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 9310 Annealed vs Normalized: Yield, Tensile & Hardness Compared.

AISI 9310 Steel Parts from Turkey

Looking for AISI 9310 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 9310 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low alloy steel grades.