300M Quenched & Tempered: Yield, Tensile & Hardness Compared

How do the 300M heat treatment properties change from one condition to another? This comparison puts the yield strength, tensile strength and hardness of 300M (UNS K44220, EN 41SiNiCrMoV7-6) side by side for 2 conditions: (High Carbon, Quenched & Tempered, (Low Carbon, Quenched & Tempered. All values are taken from the individual 300M material data sheets linked below.

300M Yield, Tensile and Hardness by Condition

ConditionYield strength (MPa)Tensile strength (MPa)Hardness (HV)Elongation (%)
(High Carbon, Quenched & Tempered1590–17501930–2130551–6097–8.14
(Low Carbon, Quenched & Tempered1520–16801860–2060551–6098–9.3

300M Differences Compared with (High Carbon, Quenched & Tempered

The table below shows how much each condition differs from the (high carbon, quenched & tempered condition, based on the mid-point of each range. Positive values mean higher strength or hardness.

ConditionYield strengthTensile strengthHardnessElongation
(Low Carbon, Quenched & Tempered-4%-3%+0%+14%

300M Strength and Hardness Charts

300M Yield strength (MPa)(High Carbon, Q&T1590–1750(Low Carbon, Q&T1520–1680
300M Tensile strength (MPa)(High Carbon, Q&T1930–2130(Low Carbon, Q&T1860–2060
300M Hardness (HV)(High Carbon, Q&T551–609(Low Carbon, Q&T551–609

300M Heat Treatment Key Points

The highest tensile strength is reached in the (high carbon, quenched & tempered condition (1930–2130 MPa). The softest condition is (high carbon, quenched & tempered (551–609 HV), which is usually preferred for machining and forming.

300M Material Data Sheets

300M (High Carbon, Quenched & Tempered | 300M (Low Carbon, Quenched & Tempered | All 300M conditions

Looking for 300M parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined 300M steel parts in-house, heat treated to the condition you specify, and inspects them before shipment.