AISI 4820 Annealed vs Normalized: Yield, Tensile & Hardness Compared

How do the AISI 4820 heat treatment properties change from one condition to another? This comparison puts the yield strength, tensile strength and hardness of AISI 4820 (UNS G48200) side by side for 2 conditions: Annealed, Normalized. All values are taken from the individual AISI 4820 material data sheets linked below.

AISI 4820 Yield, Tensile and Hardness by Condition

ConditionYield strength (MPa)Tensile strength (MPa)Hardness (HV)Elongation (%)
Annealed410–515610–750183–22318–27
Normalized435–535675–830210–26019–29

AISI 4820 Differences Compared with Annealed

The table below shows how much each condition differs from the annealed condition, based on the mid-point of each range. Positive values mean higher strength or hardness.

ConditionYield strengthTensile strengthHardnessElongation
Normalized+5%+11%+16%+7%

AISI 4820 Strength and Hardness Charts

AISI 4820 Yield strength (MPa)Annealed410–515Normalized435–535
AISI 4820 Tensile strength (MPa)Annealed610–750Normalized675–830
AISI 4820 Hardness (HV)Annealed183–223Normalized210–260

AISI 4820 Heat Treatment Key Points

The highest tensile strength is reached in the normalized condition (675–830 MPa). The softest condition is annealed (183–223 HV), which is usually preferred for machining and forming.