AISI 4620 Annealed vs Normalized: Yield, Tensile & Hardness Compared

How do the AISI 4620 heat treatment properties change from one condition to another? This comparison puts the yield strength, tensile strength and hardness of AISI 4620 (UNS G46200) side by side for 2 conditions: Annealed, Normalized. All values are taken from the individual AISI 4620 material data sheets linked below.

AISI 4620 Yield, Tensile and Hardness by Condition

ConditionYield strength (MPa)Tensile strength (MPa)Hardness (HV)Elongation (%)
Annealed330–415460–560140–17024–38
Normalized325–410515–635160–20023–35

AISI 4620 Differences Compared with Annealed

The table below shows how much each condition differs from the annealed condition, based on the mid-point of each range. Positive values mean higher strength or hardness.

ConditionYield strengthTensile strengthHardnessElongation
Normalized-1%+13%+16%-6%

AISI 4620 Strength and Hardness Charts

AISI 4620 Yield strength (MPa)Annealed330–415Normalized325–410
AISI 4620 Tensile strength (MPa)Annealed460–560Normalized515–635
AISI 4620 Hardness (HV)Annealed140–170Normalized160–200

AISI 4620 Heat Treatment Key Points

The highest tensile strength is reached in the normalized condition (515–635 MPa). The softest condition is annealed (140–170 HV), which is usually preferred for machining and forming.

AISI 4620 Material Data Sheets

AISI 4620 Annealed | AISI 4620 Normalized | All AISI 4620 conditions