AISI 4135 Normalized vs Quenched & Tempered: Yield, Tensile & Hardness Compared

How do the AISI 4135 heat treatment properties change from one condition to another? This comparison puts the yield strength, tensile strength and hardness of AISI 4135 (UNS G41350, EN 34CrMo4) side by side for 2 conditions: Normalized, Air Melted, Quenched & Tempered. All values are taken from the individual AISI 4135 material data sheets linked below.

AISI 4135 Yield, Tensile and Hardness by Condition

ConditionYield strength (MPa)Tensile strength (MPa)Hardness (HV)Elongation (%)
Normalized483–586621–690200–2408–18
Air Melted, Quenched & Tempered690–1210862–1380320–3906–12

AISI 4135 Differences Compared with Normalized

The table below shows how much each condition differs from the normalized condition, based on the mid-point of each range. Positive values mean higher strength or hardness.

ConditionYield strengthTensile strengthHardnessElongation
Air Melted, Quenched & Tempered+78%+71%+61%-31%

AISI 4135 Strength and Hardness Charts

AISI 4135 Yield strength (MPa)Normalized483–586Air Melted, Q&T690–1210
AISI 4135 Tensile strength (MPa)Normalized621–690Air Melted, Q&T862–1380
AISI 4135 Hardness (HV)Normalized200–240Air Melted, Q&T320–390

AISI 4135 Heat Treatment Key Points

The highest tensile strength is reached in the air melted, quenched & tempered condition (862–1380 MPa). The softest condition is normalized (200–240 HV), which is usually preferred for machining and forming.

AISI 4135 Material Data Sheets

AISI 4135 Normalized | AISI 4135 Air Melted, Quenched & Tempered | All AISI 4135 conditions

Looking for AISI 4135 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 4135 steel parts in-house, heat treated to the condition you specify, and inspects them before shipment.